Thermal Properties Metric English Comments
Maximum Service Temperature, Air 334 °C
633 °F
NEXA® PFX9014 Perfluoroelastomer
NEXA produces sealing elements for extreme and critical applications, particularly where high temperature, wet conditions (steam/water), purity and chemical resistance are important factors to consi..