Thermal Properties | Metric | English | Comments |
---|---|---|---|
Maximum Service Temperature, Air | 500 - 600 °C | 932 - 1110 °F | Continuous |
Goodfellow Potassium Aluminosilicate (Muscovite Mica) Mica is a naturally occurring mineral and as such its exact composition varies between grades, as will its properties. Ruby Mica is the highest grade of Muscovite Mica. The name comes from the Latin.. |