Thermal Properties | Metric | English | Comments |
---|---|---|---|
Maximum Service Temperature, Air | 470 °C | 878 °F | Continuous |
Pyrotek F-24 Dense Machinable Board F-24 is a high temperature resin material that is reinforced with fiberglass. Abrasion resistant, it is used for hot glass handling applications.ApplicationsDonut rollers for glass Guide rails Wear.. |
|||
Maximum Service Temperature, Air | 470 °C | 878 °F | Heat Distortion Temp, Load Unknown; ASTM D648 |
UBE UPIMOL® SA101 Heat-Resistant Polyimide Shape Description: UPIMOL® SA101 is an excellent heat-resistant polyimide shape, based on Biphenyl tetracarboxilic dianhydride(BPDA) originally developed by UBE. UPIMOL® SA101 has improved high durabili.. |