Thermal Properties | Metric | English | Comments |
---|---|---|---|
Maximum Service Temperature, Air | 225 °C | 437 °F | Recommended |
Nye Lubricants 436 (SO) Synthetic Oil Information provided by Nye Lubricants. |
|||
Maximum Service Temperature, Air | 225 °C | 437 °F | Recommended |
Nye Lubricants 570H-10 (NT) Synthetic Oil Information provided by Nye Lubricants. |
|||
Maximum Service Temperature, Air | 225 °C | 437 °F | Recommended |
Nye Lubricants 570H-25 (NT) Synthetic Oil Information provided by Nye Lubricants. |
|||
Maximum Service Temperature, Air | 225 °C | 437 °F | Recommended |
Nye Lubricants UniFlor 8170 (UF) Synthetic Oil Information provided by Nye Lubricants. |
|||
Maximum Service Temperature, Air | 225 °C | 437 °F | Recommended |
Nye Lubricants UniFlor 8172R (829RP) (UF) Synthetic Oil Information provided by Nye Lubricants. |
|||
Maximum Service Temperature, Air | 225 °C | 437 °F | Recommended |
Nye Lubricants UniFlor 8180 (479) (UF) Synthetic Oil Information provided by Nye Lubricants. |
|||
Maximum Service Temperature, Air | 225 °C | 437 °F | Recommended |
Nye Lubricants UniFlor 8182 (837) (UF) Synthetic Oil Information provided by Nye Lubricants. |
|||
Maximum Service Temperature, Air | 225 °C | 437 °F | Recommended |
Nye Lubricants UniFlor 8511E (853-2EP) (UF) Synthetic Oil Information provided by Nye Lubricants. |
|||
Maximum Service Temperature, Air | 225 °C | 437 °F | Recommended |
Nye Lubricants UniFlor 8511U (UF) Synthetic Oil Information provided by Nye Lubricants. |
|||
Maximum Service Temperature, Air | 225 °C | 437 °F | Recommended |
Nye Lubricants UniFlor 8512F (842G0) (UF) Synthetic Oil Information provided by Nye Lubricants. |
|||
Maximum Service Temperature, Air | 225 °C | 437 °F | Recommended |
Nye Lubricants UniFlor 8512-FG (UF) Synthetic Oil Information provided by Nye Lubricants. |
|||
Maximum Service Temperature, Air | 225 °C | 437 °F | Recommended |
Nye Lubricants UniFlor 8512R (842RP) (UF) Synthetic Oil Information provided by Nye Lubricants. |
|||
Maximum Service Temperature, Air | 225 °C | 437 °F | Recommended |
Nye Lubricants UniFlor 8512S (842S) (UF) Synthetic Oil Information provided by Nye Lubricants. |
|||
Maximum Service Temperature, Air | 225 °C | 437 °F | Recommended |
Nye Lubricants UniFlor 8521R (841RP-1) (UF) Synthetic Oil Information provided by Nye Lubricants. |
|||
Maximum Service Temperature, Air | 225 °C | 437 °F | Recommended |
Nye Lubricants UniFlor 8531 (834-1) (UF) Synthetic Oil Information provided by Nye Lubricants. |
|||
Maximum Service Temperature, Air | 225 °C | 437 °F | Recommended |
Nye Lubricants UniFlor 8531R (834RP-1) (UF) Synthetic Oil Information provided by Nye Lubricants. |
|||
Maximum Service Temperature, Air | 225 °C | 437 °F | Recommended |
Nye Lubricants UniFlor 8910 (490) (UF) Synthetic Oil Information provided by Nye Lubricants. |
|||
Maximum Service Temperature, Air | 225 °C | 437 °F | |
Precision Polymer Engineering F60A Fluorosilicone Rubber Blue Fluorosilicone, 56-65 °IRHD. Fluorosilicone rubber having methyl, vinyl and fluorine substituent groups on the polymer chain. To meet Aerospace Specification Mil-R-25988B, Class 1, Grade 60... |
|||
Maximum Service Temperature, Air | 225 °C | 437 °F | |
Precision Polymer Engineering V90D Fluoroelastomer Compound Fluoroelastomer Rubber, 86-93 °IRHD. Copolymer of vinylidene fluoride and hexafluoropropylene. Meets Aerospace Specifications DTD5612A and DTD5543B Grade 90. ASTM designation = FKM. ISO designatio.. |
|||
Maximum Service Temperature, Air | 225 °C | 437 °F | |
LATI Larpeek 10 K/20 PEEK, 20% Carbon Fiber Reinforced Polyetheretherketone (PEEK) based compound. Carbon fiber. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa & Middle East; As.. |
|||
Maximum Service Temperature, Air | 225 °C | 437 °F | |
LATI Larton K/30 PPS, 30% Carbon Fiber Reinforced Polyphenylene Sulfide (PPS) based compound. Carbon fiber. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa & Middle East; As.. |
|||
Maximum Service Temperature, Air | 225 °C | 437 °F | |
LATI Laticonther 80 GCE/650 PPS, Glass/Mineral Reinforced High thermal conductivity product based on Polyphenylene Sulfide (PPS). Glass fibers / Mineral filler.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformatio.. |
|||
Maximum Service Temperature, Air | 225 °C | 437 °F | Ball pressure temperature; IEC Method |
Toyobo VYLOPET® EMC532 Injection Molding Polyester Resin, Glass Reinforced Applications: Auto-partsFeatures: Ultrasonic weldabilityGlass fiber reinforcementInformation provided by Toyobo. |
|||
Maximum Service Temperature, Air | 225 °C | 437 °F | Continuous |
Epoxy Technology EPO-TEK® H20E-PFC Electrically Conductive, Silver Epoxy Product Description: EPO-TEK® H20E-PFC is a two component, semiconductor grade epoxy, designed for flip chip interconnects using a solder-free joining method.Advantages & Application Notes: Stencil.. |
|||
Maximum Service Temperature, Air | 225 °C | 437 °F | Continuous |
Epoxy Technology EPO-TEK® H54 High Temperature Epoxy Product Description: EPO-TEK® H54 is a two component, high Tg, electrically and thermally insulating epoxy adhesive for general bonding and high temperature packaging in medical, hybrid, and optica.. |
|||
Maximum Service Temperature, Air | 225 °C | 437 °F | Continuous |
Epoxy Technology EPO-TEK® U300-2 Two Component Epoxy Material Description: A two component epoxy designed for capillary underfill of semiconductor chips and SMDs. Long potlife, high Tg, and optical clarity are a few of its traits. NASA approved lo.. |
|||
Maximum Service Temperature, Air | 225 °C | 437 °F | Recommended |
Nye Lubricants UniFlor 8911R (891RP-1) (UF) Synthetic Oil Information provided by Nye Lubricants. |
|||
Maximum Service Temperature, Air | 225 °C | 437 °F | Recommended |
Nye Lubricants UniFlor 8917 (UF) Synthetic Oil Information provided by Nye Lubricants. |
|||
Maximum Service Temperature, Air | 225 °C | 437 °F | Heat Resistance; ASTM D570D |
Plenco 7552 Phenolic, Nodular, Transfer Molded PLENCO 07552 is a glass fiber reinforced novolac phenolic molding compound, exhibiting superior dimensional stability, good impact strength, and good electrical properties. Type ASTM 5948 MFH. UL re.. |