Thermal Properties | Metric | English | Comments |
---|---|---|---|
Maximum Service Temperature, Air | <= 176 °C | <= 349 °F | short time use temperature |
Honeywell Capran® Oxyshield™ OXTR (Retortable Grade, 0.6 mil) Monoaxially Oriented Co-Extruded Nylon 6/EVOH/Nylon 6 Clear Film Description: Capran® Oxyshield™ Oriented Ultra Barrier Retortable Grade is a monoaxially oriented, co-extruded nylon 6-based clear film having excellent gas barrier through a broad range of .. |
|||
Maximum Service Temperature, Air | <= 176 °C | <= 349 °F | short time use temperature |
Honeywell Capran® Oxyshield™ OXTR (Retortable Grade, 1.0 mil) Monoaxially Oriented Co-Extruded Nylon 6/EVOH/Nylon 6 Clear Film Description: Capran® Oxyshield™ Oriented Ultra Barrier Retortable Grade is a monoaxially oriented, co-extruded nylon 6-based clear film having excellent gas barrier through a broad range of .. |
|||
Maximum Service Temperature, Air | <= 176 °C | <= 349 °F | Continuous Use |
Arlon CuClad 6700 Bonding Film Thermoplastic Bonding FilmsSimilar Dk and Df range to many PTFE laminatesBenefits:Can be reheated to remelt and reflow bonding filmExcellent Electrical PropertiesTypical Applications:Stripline Circu.. |
|||
Maximum Service Temperature, Air | 176 °C | 349 °F | |
3M Scotch® 22 Heavy Duty Vinyl Electrical Tape Scotch® Heavy Duty Vinyl Electrical Tape 22 is a premium grade, 10 mil thick, vinyl chloride tape. It is designed to perform continuously in ambient temperatures up to 80°C. The tape is conformabl.. |
|||
Maximum Service Temperature, Air | 176 °C | 349 °F | |
3M Temflex™ 1700 Vinyl Electrical Tape Scotch® Vinyl Electrical Tape 1700 is a good quality, economical general purpose vinyl insulating tape. It has excellent resistance to: abrasion, moisture, alkalies, acid, copper corrosion and vary.. |
|||
Maximum Service Temperature, Air | 176 °C | 349 °F | |
Rogers Corporation 3001 Thermoplastic Chloro-Fluorocopolymer Bonding Film Rogers 3001 bonding film is a thermoplastic chloro-fluorocopolymer. It is recommended for bonding low dielectric constant PTFE (Teflon® fluorocarbon polymer) microwave stripline packages and other.. |