Thermal Properties | Metric | English | Comments |
---|---|---|---|
Maximum Service Temperature, Air | 166 °C | 330 °F | UL-746 B |
Saint-Gobain Norton® ETFE Fluoropolymer Film Features/Benefits:Superior release propertiesExcellent weatherabilityPerformance from -200°C (-328°F) to 165°C (330°F)Excellent chemical and mechanical propertiesThermoformableProduct th.. |
|||
Maximum Service Temperature, Air | 166 °C | 330 °F | Intermittent |
Ensinger Tecast Vekton™ 6PAG Graphite-Filled Cast Nylon 6 (PA6) Tecast® 6PAG is a graphite powder-filled with properties similar to MoS2-filled but better suited to wet applications.General Tecast® Cast Nylon Information: Tecast cast nylon, available in a vari.. |
|||
Maximum Service Temperature, Air | 166 °C | 330 °F | Intermittent |
Ensinger Tecast Vekton™ 6PALM Premium Bearing Grade cast nylon (PA6) Tecast 6PALM contains both solid and liquid lubricants dispersed throughout the nylon to provide consistent wear rates and coefficients of friction.Information provided by Ensinger, Inc. |
|||
Maximum Service Temperature, Air | 166 °C | 330 °F | Intermittent |
Cast Nylons Nycast® GF 30% Glass Filled Cast Nylon Offering improved tensile, compressive and flexural properties over conventional unfilled cast nylon, NYCAST® GF (Glass Filled)-30% provides increased load bearing characteristics and is the choice.. |
|||
Maximum Service Temperature, Air | 166 °C | 330 °F | Intermittent |
Cast Nylons Nycast® GX Solid Lubricant Filled Gray Cast Nylon 6 NYCAST® GX is a specially formulated, self-lubricating grade designed to deliver low coefficient of friction, superior wear resistance, high pressure/velocity performance, and low moisture absorpti.. |
|||
Maximum Service Temperature, Air | 166 °C | 330 °F | Intermittent |
Cast Nylons Nycast® RX Solid Lubricant Filled Red Cast Nylon 6 NYCAST® RX is a specially formulated, self-lubricating grade designed to deliver low coefficient of friction, superior wear resistance, high pressure/velocity performance, and low moisture absorpti.. |