Thermal Properties | Metric | English | Comments |
---|---|---|---|
Maximum Service Temperature, Air | 32.2 - 343 °C | 90.0 - 650 °F | Average value: 143 °C Grade Count:176 |
Overview of materials for Epoxy Encapsulant, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Epoxy Encapsulant, Unreinforced". Each property range of values reported is minimum and maximum values o.. |
|||
Maximum Service Temperature, Air | 32.2 °C | 90.0 °F | |
Spartech WI50D34SR PVC and Alloy Products for Wire and Cable Information provided by Spartech |
|||
Maximum Service Temperature, Air | 32.2 °C | 90.0 °F | |
Spartech WI8940FR-90 PVC and Alloy Products for Wire and Cable Information provided by Spartech |
|||
Maximum Service Temperature, Air | 32.2 °C | 90.0 °F | |
Master Bond EP21FRNS-2 Two Component, Flame Resistant Epoxy System Master Bond Polymer System EP21FRNS-2 is a two component, room temperature curing, flame retardant compound for potting, encapsulating and casting. Particularly noteworthy are its low smoke generati.. |