Thermal Properties Metric English Comments
Maximum Service Temperature, Air 1425 °C
2597 °F
ICE Steatite L-4
Data provided by the manufacturer, International Ceramic Engineering.
Maximum Service Temperature, Air 1425 °C
2597 °F
ICE Steatite L-5
Data provided by the manufacturer, International Ceramic Engineering.
Maximum Service Temperature, Air 1425 °C
2597 °F
Gouda Vuurvast GI 26 Insulating Refractory Brick
This data represents average values, obtained from samples that were cut from standard bricks.Information provided by Gouda Vuurvast.
Maximum Service Temperature, Air 1425 °C
2597 °F
Sharadaa Ceramics Blankets
Services Offered: Retrofitting of Furnace, Installation of Castables/Bricks/Ceramic Fiber Modules, Castable Laying by Vibrocasting/Guiniting, Turnkey Installation Boiler/Chimney/Heater/Reformer/Rota..
Maximum Service Temperature, Air 1425 °C
2597 °F
Zircar Ceramics HITAC-4 High Alumina Refractory Adhesive
High Alumina Refractory Adhesive Type HITAC-4 is a single part water based high alumina containing adhesive. Specifically developed for bonding low-density fibrous ceramic insulation materials toge..
Maximum Service Temperature, Air 1425 °C
2597 °F
Chesterton 725 Nickel Anti-Seize Compound
Description: Chesterton® 725 Nickel Anti-Seize Compound is an assembly lubricant combining the extreme pressure, corrosion resistant anti-seize abilities of colloidal nickel, aluminum and graphite ..
Maximum Service Temperature, Air 1425 °C
2597 °F
Chesterton 772 Premium Nickel Anti-Seize Compound
Description: Chesterton® 772 Premium Nickel Anti-Seize Compound is formulated with ultra pure raw materials. This permits 772 Premium Nickel Anti-Seize Compound to conform to most applicable equipm..