Thermal Properties Metric English Comments
Maximum Service Temperature, Air 198 °C
388 °F
Heat resistance per ASTM D794
Plenco 7300 Phenolic, Nodular, Injection Molded  (discontinued **)
Two-Stage Phenolic. PLENCO 07300 is an organic fiber reinforced phenolic molding compound offering improved mechanical strength and excellent cosmetic properties. UL recognized under component file..
Maximum Service Temperature, Air 198 °C
388 °F
Heat Resistance; ASTM D570D
Plenco 2000 Phenolic, Granular, Injection Molded
PLENCO 02000 is a versatile general purpose, organic filled phenolic molding compound, offering optimum cure characteristics and an excellent balance of molding properties. UL recognized under compo..
Maximum Service Temperature, Air 198 °C
388 °F
Heat Resistance; ASTM D570D
Plenco 7697 Phenolic, Granular, Compression Molded
PLENCO 07697 is a black, two stage, improved impact phenolic molding compound. It has been specifically formulated for automotive pulleys. PLENCO 07697 is the same formulation as VALITE 697-A.Inform..