Thermal Properties | Metric | English | Comments |
---|---|---|---|
Maximum Service Temperature, Air | 1425 °C | 2597 °F | |
ICE Steatite L-4 Data provided by the manufacturer, International Ceramic Engineering. |
|||
Maximum Service Temperature, Air | 1425 °C | 2597 °F | |
ICE Steatite L-5 Data provided by the manufacturer, International Ceramic Engineering. |
|||
Maximum Service Temperature, Air | 1425 °C | 2597 °F | |
Gouda Vuurvast GI 26 Insulating Refractory Brick This data represents average values, obtained from samples that were cut from standard bricks.Information provided by Gouda Vuurvast. |
|||
Maximum Service Temperature, Air | 1425 °C | 2597 °F | |
Sharadaa Ceramics Blankets Services Offered: Retrofitting of Furnace, Installation of Castables/Bricks/Ceramic Fiber Modules, Castable Laying by Vibrocasting/Guiniting, Turnkey Installation Boiler/Chimney/Heater/Reformer/Rota.. |
|||
Maximum Service Temperature, Air | 1425 °C | 2597 °F | |
Zircar Ceramics HITAC-4 High Alumina Refractory Adhesive High Alumina Refractory Adhesive Type HITAC-4 is a single part water based high alumina containing adhesive. Specifically developed for bonding low-density fibrous ceramic insulation materials toge.. |
|||
Maximum Service Temperature, Air | 1425 °C | 2597 °F | |
Chesterton 725 Nickel Anti-Seize Compound Description: Chesterton® 725 Nickel Anti-Seize Compound is an assembly lubricant combining the extreme pressure, corrosion resistant anti-seize abilities of colloidal nickel, aluminum and graphite .. |
|||
Maximum Service Temperature, Air | 1425 °C | 2597 °F | |
Chesterton 772 Premium Nickel Anti-Seize Compound Description: Chesterton® 772 Premium Nickel Anti-Seize Compound is formulated with ultra pure raw materials. This permits 772 Premium Nickel Anti-Seize Compound to conform to most applicable equipm.. |