Thermal Properties | Metric | English | Comments |
---|---|---|---|
Maximum Service Temperature, Air | 1300 °C | 2370 °F | |
Gouda Vuurvast ADHESIET B Dry Air-Setting Refractory Mortar Description: Adhesiet B is a general purpose air setting mortar, supplied as a dry powder for use up to 1300°C.Remarks: Adhesiet mortars can be stored for an unlimited time if kept dry and cool. .. |
|||
Maximum Service Temperature, Air | 1300 °C | 2370 °F | |
Gouda Vuurvast B Sp Dense Refractory Brick Description: A very dense brick, high resistance against slag penetration. Application: in rotary kilns (cement) and incinerators.Remarks: This data represents average values, obtained from samples .. |
|||
Maximum Service Temperature, Air | 1300 °C | 2370 °F | |
Gouda Vuurvast CURON 130 Dense Refractory Castable Description: Curon 130 is a castable with a good workability and a high strength. Therefore this castable can be characterized as a reliable refractory construction material.Remarks: These values ap.. |
|||
Maximum Service Temperature, Air | 1300 °C | 2370 °F | Deformation under load - t<sub>a</sub> |
Gouda Vuurvast AK 85 PW Dense Refractory Brick Description: A phosphate bonded bauxite brick with outstanding erosion resistance and resistance against liquid aluminum. Application: aluminum holding furnaces.Remarks: This data represents average.. |
|||
Maximum Service Temperature, Air | 1300 °C | 2370 °F | |
Gouda Vuurvast CURON 13 S Dense Refractory Castable Description: Curon 13 S is a spinel based castable with a very low silica content and therefore it is suitable for direct contact with all kinds of aluminum/alloys and fluxes in aluminum melting/hol.. |
|||
Maximum Service Temperature, Air | 1300 °C | 2370 °F | |
Gouda Vuurvast CURON 130 HRC AL Dense Refractory Castable Description: Because of special addition this castable is used for the walls above the liquid level in aluminum melting furnaces.Remarks: These values apply to cast products.Information provided by .. |
|||
Maximum Service Temperature, Air | 1300 °C | 2370 °F | |
Gouda Vuurvast CURON 130 HRC Dense Refractory Castable Description: A coarse, low iron castable for use up to 1300°C under normal operation conditions, also usable under reducing circumstances. Curon 130 HRC has a good thermal shock resistance becaus.. |
|||
Maximum Service Temperature, Air | 1300 °C | 2370 °F | |
Gouda Vuurvast CURON 130 HRCC RAPID Dense Refractory Castable Description: An extra coarse, low iron castable for use to 1300°C under normal operation conditions, also usable under reducing circumstances. Curon 130 HRCC RAPID has good thermal shock resistan.. |
|||
Maximum Service Temperature, Air | 1300 °C | 2370 °F | |
Gouda Vuurvast GOLITE 130 GM Refractory Insulating Castable Description: Golite 130 GM is a standard, medium weight gunning castable, combining a good mechanical strength with a low density and a low thermal conductivity.Remarks: These values apply to cast p.. |
|||
Maximum Service Temperature, Air | 1300 °C | 2370 °F | |
Sharadaa Ceramics HFI Insulation Brick Services Offered: Retrofitting of Furnace, Installation of Castables/Bricks/Ceramic Fiber Modules, Castable Laying by Vibrocasting/Guiniting, Turnkey Installation Boiler/Chimney/Heater/Reformer/Rota.. |
|||
Maximum Service Temperature, Air | 1300 °C | 2370 °F | |
Sharadaa Ceramics REFCAST NORMAL Dense Castables Description: We offer a range of Dense Castables that are conventional castable and extensively used in boiler work, general furnace and burner blocks. Made as per international standards, our range.. |
|||
Maximum Service Temperature, Air | 1300 °C | 2370 °F | |
Sharadaa Ceramics Sharada LTM 0.7 Insulating Castable Low Density/ High Strength Insulating Castable-Low Thermal Mass LiningInformation provided by Sharadaa Ceramics Pvt. Ltd. |
|||
Maximum Service Temperature, Air | 1300 °C | 2370 °F | |
Sharadaa Ceramics Sharada LTM 0.9 Insulating Castable Low Density/ High Strength Insulating Castable-Low Thermal Mass LiningInformation provided by Sharadaa Ceramics Pvt. Ltd. |
|||
Maximum Service Temperature, Air | 1300 °C | 2370 °F | Deformation temp |
SPHERE ONE EXTENDOSPHERESâ„¢ 350 Hollow Spheres EXTENDOSPHERESâ„¢ hollow spheres are efficient, lightweight additives for most resin systems. When Extendospheresâ„¢ replace heavier, more expensive components on an equivalent volume basis, t.. |
|||
Maximum Service Temperature, Air | 1300 °C | 2370 °F | Deformation temp |
SPHERE ONE EXTENDOSPHERESâ„¢ CG Hollow Spheres EXTENDOSPHERESâ„¢ hollow spheres are efficient, lightweight additives for most resin systems. When Extendospheresâ„¢ replace heavier, more expensive components on an equivalent volume basis, t.. |
|||
Maximum Service Temperature, Air | 1300 °C | 2370 °F | Deformation temp |
SPHERE ONE EXTENDOSPHERESâ„¢ MG Hollow Spheres EXTENDOSPHERESâ„¢ hollow spheres are efficient, lightweight additives for most resin systems. When Extendospheresâ„¢ replace heavier, more expensive components on an equivalent volume basis, t.. |
|||
Maximum Service Temperature, Air | 1300 °C | 2370 °F | Deformation temp |
SPHERE ONE EXTENDOSPHERESâ„¢ TG Hollow Spheres EXTENDOSPHERESâ„¢ hollow spheres are efficient, lightweight additives for most resin systems. When Extendospheresâ„¢ replace heavier, more expensive components on an equivalent volume basis, t.. |
|||
Maximum Service Temperature, Air | 1300 °C | 2370 °F | |
CeramTec Rubalit® IS 95 Alumina Rubalit® IS 95 is a high-performance alumina ceramic. Aluminas exhibit good mechanical properties such as hardness, compressive and tensile strength, and elastic modulus. They perform well at eleva.. |
|||
Maximum Service Temperature, Air | 1300 °C | 2370 °F | |
CeramTec SL 200 BG Silicon Nitride, Si3N4-Y2O3 SL 200 BG is a silicon nitride ceramic used to make welding rollers, pins, and components, gas nozzles, and forming tools. Silicon nitrides are ideal for components working under mechanical loads an.. |
|||
Maximum Service Temperature, Air | 1300 °C | 2370 °F | |
Zircar Ceramics AX-200 Refractory Supported Heater ZIRCAR Refractory Supported Heater Type AX-200 consists of high temperature, helically-wound, iron-chrome-aluminum metallic alloy resistance heating elements fully embedded in a strong, highly stabl.. |
|||
Maximum Service Temperature, Air | 1300 °C | 2370 °F | |
Zircar Refractory Composites RS-Cloth Refractory Sheet Refractory Sheet RS-Cloth is ceramic fiber reinforced alumina composite. It offers the strength, durability, flexibility and versatility required by many high temperature applications up to 1300°C(.. |
|||
Maximum Service Temperature, Air | 1300 °C | 2370 °F | |
Zircar Refractory Composites RS-1200 Refractory Sheet ZIRCAR Refractory Sheet Type RS-1200 is a high strength composite designed for use as thermo-mechanical and electrical insulation in applications with temperatures as high as 1300°C(2372°F). RS-12.. |
|||
Maximum Service Temperature, Air | 1300 °C | 2370 °F | limited |
Chosun Refractories CT-130 Fireclay Castables Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Maximum Service Temperature, Air | 1300 °C | 2370 °F | |
BNZ Materials BNZP-23B Insulating Firebrick (French Grade) BNZ produces many types of Insulating Fire Brick (IFB) for use in applications from 2,000°F (1,093°C) to 3,200°F (1,760°C). Each type is formulated to meet specific thermal and physical requirem.. |
|||
Maximum Service Temperature, Air | 1300 °C | 2370 °F | limited |
Chosun Refractories PTC-130S Plastic Refractory Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |