Thermal Properties Metric English Comments
Maximum Service Temperature, Air 117 °C
243 °F
Heat deflection temperature, load unknown; ASTM D648
Toyobo PELPRENE™ P150B Polyester TPE
Features: Polyester TPEInformation provided by Toyobo.
Maximum Service Temperature, Air 117 °C
243 °F
Heat deflection temperature, load unknown; ASTM D648
Toyobo PELPRENE™ P150B-05 Polyester TPE, Non-smell, Non-deposit
Features: Polyester TPE, Non-smell, Non-depositInformation provided by Toyobo.
Maximum Service Temperature, Air 117 °C
243 °F
Heat deflection temperature, load unknown; ASTM D648
Toyobo PELPRENE™ S3001 Polyester TPE
Features: Polyester TPEInformation provided by Toyobo.
Maximum Service Temperature, Air 117 °C
243 °F
Heat deflection temperature, load unknown; ASTM D648
Toyobo PELPRENE™ S3002 Polyester TPE, Ultra Heat-resistant
Features: Polyester TPE, Ultra Heat-resistantInformation provided by Toyobo.
Maximum Service Temperature, Air 117 °C
243 °F
3M 230 Crystal Clear Sealant
3M™ Crystal Clear Sealant 230 is a one component thermoplastic elastomer which forms permanent elastic bonds when used in surface sealing applications. 3M Crystal Clear Sealant 230 bonds to a wide ..