Thermal Properties | Metric | English | Comments |
---|---|---|---|
Maximum Service Temperature, Air | 1050 °C | 1920 °F | |
Pyrotek ISOMAG® 175 Structural Insulation Board Isomag® 70 is a high strength insulating board suitable as an electrical insulator or a thermal barrier material in a variety of industrial applications. Its magnesia silicate based formulation pr.. |
|||
Maximum Service Temperature, Air | 1050 °C | 1920 °F | |
Pyrotek ISOMAG® 70 Structural Insulation Isomag® 70 is magnesia silicate based formulation provides insulating properties similar to calcium silicate with good strength and dimensional stability up to 1000°C. ApplicationsTorpedo cars La.. |
|||
Maximum Service Temperature, Air | 1050 °C | 1920 °F | |
MetalTek MTEK 25-35 Cast UNS N08705; Cast UNS J95705 Heat Resistant Stainless Steel Higher chrome and nickel content provides increased strength and resistance to both oxidation and carburization.Applications: Reformer and Ethylene pyrolysis tubes and fittings.Information provided .. |
|||
Maximum Service Temperature, Air | 1050 °C | 1920 °F | Normal Conditions |
Saint-Gobain HS Grade Optical Fused Quartz HS Grade Optical Fused Quartz is a high purity, low [OH] natural fused quartz. It has excellent IR transmission, useful transmission from 260 to 3500 nm, excellent visual quality with low bubbles, .. |
|||
Maximum Service Temperature, Air | 1050 °C | 1920 °F | |
Saint-Gobain Quartzel® Fused Quartz Textiles Quartzel® fiber is produced from quartz crystal that is ground, purified, fiberized by a fusion process. It is homogeneous, non-porous, continuous, amorphous, ultra pure silica glass. It is ava.. |
|||
Maximum Service Temperature, Air | 1050 °C | 1920 °F | Normal Conditions |
Saint-Gobain Spectrosil® 1000 Optical Fused Quartz Spectrosil® 1000 grade is used for non-transmissive mirrors and substrates, and other high purity components which do not require specified optical transmission.Spectrosil® is a synthetic fuse.. |
|||
Maximum Service Temperature, Air | 1050 °C | 1920 °F | Normal Conditions |
Saint-Gobain Spectrosil® 2000 Optical Fused Quartz Spectrosil® 2000 is a deep UV, fluorescence-free grade.Spectrosil® is a synthetic fused silica manufactured using a patented, environmentally friendly process that results in a virtually chlor.. |
|||
Maximum Service Temperature, Air | 1050 °C | 1920 °F | Normal Conditions |
Saint-Gobain Spectrosil® 2100 Optical Fused Quartz Spectrosil® 2100 has improved refractive index homogeneity.Spectrosil® is a synthetic fused silica manufactured using a patented, environmentally friendly process that results in a virtually c.. |
|||
Maximum Service Temperature, Air | 1050 °C | 1920 °F | Normal Conditions |
Saint-Gobain Spectrosil® 2200 Optical Fused Quartz Spectrosil® 2200 grade is an excimer laser grade developed for maximum transmission and prolonged life in microlithography and other critical deep UV applications using KrF (248 nm) and ArF (193 .. |
|||
Maximum Service Temperature, Air | 1050 °C | 1920 °F | Normal Conditions |
Saint-Gobain Vitreosil® 055 Optical Fused Quartz Vitreosil® 055 is the highest grade of optical grade fused quartz available from Saint-Gobain Quartz for use in the near UV and visible. It has a useful transmission range from 270 nm in the nea.. |
|||
Maximum Service Temperature, Air | 1050 °C | 1920 °F | Normal Conditions |
Saint-Gobain Vitreosil® 065 066 Optical Fused Quartz Vitreosil® 065, for use in the near UV and visible, has a less rigorous bubble specification. It has a useful transmission range from 270 nm in the near UV to 2000 nm in the IR.Vitreosil® opt.. |
|||
Maximum Service Temperature, Air | 1050 °C | 1920 °F | Normal Conditions |
Saint-Gobain Vitreosil® Clear Fused Quartz Tubing Electrically fused quartz is recognized for its combination of purity, chemical inertness, physical stability, thermal shock resistance, high electrical resistivity, and high operating temperatures... |
|||
Maximum Service Temperature, Air | 1050 °C | 1920 °F | |
Skamol Group VERMICAST 116-25 Insulating Castable SKAMOL insulating castables have the following characteristics: Max. service temperature: Up to 1100°C (2102°F)Back-up insulation or hot-face usesFor casting and gunningProducts are based on f.. |
|||
Maximum Service Temperature, Air | 1050 °C | 1920 °F | Normal Conditions |
Saint-Gobain Puropsil® B Infrared Grade Low [OH] Optical Fused Quartz Puropsil® B optical infrared fused quartz is manufactured from naturally occurring quartz crystal using a plasma process to ensure a low OH. It has excellent IR transmission with a useful IR tra.. |
|||
Maximum Service Temperature, Air | 1050 °C | 1920 °F | Normal Conditions |
Saint-Gobain Vitreosil® CFQ/TSC Optical Fused Quartz Vitreosil® CFQ/TSC grades are for use in less demanding applications including viewing windows for use in corrosive and high temperature environments and non-optical components such as spacers, i.. |
|||
Maximum Service Temperature, Air | 1050 °C | 1920 °F | continuous, core material |
Unifrax Excelfrax® 1900 Panel Microporous Insulation Unifrax Corporation's Excelfrax® product line, based on advanced microporous insulation technology, is a family of products which all exhibit superior insulating characteristics. Excelfrax micropo.. |
|||
Maximum Service Temperature, Air | 1050 °C | 1920 °F | |
Goodfellow Leachable Ceramic (Silica, Zircon, Alumina) SiO2 50/ZrSiO4 40/Al2O3 10This form of ceramic is used in the precision foundry industry. The tubes and rods are incorporated into molds in the lost wax process. Using this technique, very fine tole.. |
|||
Maximum Service Temperature, Air | 1050 °C | 1930 °F | Peak |
AK Steel 18 SR® Ferritic Stainless steel AK Steel 18 SR® provides excellent resistance to high temperature scaling - far superior to that of Type 446 stainless steel. This material is readily welded by conventional methods. It is not su.. |