Thermal Properties | Metric | English | Comments |
---|---|---|---|
Maximum Service Temperature, Inert | 210 °C @Thickness 0.000 mm, Time 7.20e+7 sec |
410 °F @Thickness 0.000 in, Time 20000 hour |
IEC 60216; IEC/EN 60893-2 7.1 |
Elektro-Isola G-Etronax SI Silicone, Glass Fabric Reinforcement, White, Sheets Description: Electrical and electrotechnical applications. Suitable as high-frequency insulation on account of its dielectric loss. Used as, among other things, an insulation material in large induc.. |
|||
Maximum Service Temperature, Inert | 210 °C @Thickness 3.00 mm, Time 7.20e+7 sec |
410 °F @Thickness 0.118 in, Time 20000 hour |
IEC 60695-11-10; IEC/EN 61212-2 7.1 |
Elektro-Isola G-Etronax SI Silicone, Glass Fabric Reinforcement, White, Tubes Description: Used in mechanical, electrical and electronic applications at elevated temperatures. Retains good electrical properties at high temperatures. Self-extinguishing. Low dielectric loss fac.. |