Thermal Properties | Metric | English | Comments |
---|---|---|---|
Maximum Service Temperature, Inert | 130 °C | 266 °F | |
Haysite H722 Polyester, Glass Reinforced H722 is an all-purpose GPO-1 fiberglass mat reinforced thermoset polyester molded sheet. Available in thicknesses ranging from .031" - 2.00". Standard color - Natural. Meets Gov't Specs - LP-509, .. |
|||
Maximum Service Temperature, Inert | 130 °C | 266 °F | ASTM D794 |
Techmer ES Plastiblend® TPX-HTN-000AA Availability: North AmericaForms: Pellets Features: High Heat ResistanceInformation provided by TP Composites, Inc. |
|||
Maximum Service Temperature, Inert | 130 °C @Thickness 3.00 mm, Time 7.20e+7 sec |
266 °F @Thickness 0.118 in, Time 20000 hour |
IEC 60695-11-10; IEC/EN 61212-2 7.1 |
Elektro-Isola Etronax DN Phenolic, Cotton Fabric Reinforcement, Brown, Tubes Description: A strong and tough material. Very low water absorption and the lowest swelling in water. Very good low-friction material. High wear resistance in aggressive and dust-filled environments.. |
|||
Maximum Service Temperature, Inert | 130 °C @Thickness 0.000 mm, Time 7.20e+7 sec |
266 °F @Thickness 0.000 in, Time 20000 hour |
IEC 60216; IEC/EN 60893-2 7.1 |
Elektro-Isola Etronax P EP Phenolic, Polyester Fabric Reinforcement, Light Yellow, Sheets Description: This material is exceptionally strong and tough. Very low water absorption and the lowest swelling in water. High resistance to chemicals, including SF6 gas. Applications: Can be used i.. |
|||
Maximum Service Temperature, Inert | 130 °C @Thickness 0.000 mm, Time 7.20e+7 sec |
266 °F @Thickness 0.000 in, Time 20000 hour |
IEC 60216; IEC/EN 60893-2 7.1 |
Elektro-Isola G-Etronax M Melamine, Glass Fabric Reinforcement, White, Sheets Description: Melamine-based composite material reinforced with glass fabric. High arc resistance and tracking resistance. Flame-resistant. Self-extinguishing.Information provided by Elektro-Isola |
|||
Maximum Service Temperature, Inert | 130 °C @Thickness 3.00 mm, Time 7.20e+7 sec |
266 °F @Thickness 0.118 in, Time 20000 hour |
IEC 60695-11-10; IEC/EN 61212-2 7.1 |
Elektro-Isola G-Etronax M Melamine, Glass Fabric Reinforcement, White, Tubes Description: Mechanical and electrical applications. Arc-resistant and tracking-resistant material. Good flame resistance. Self-extinguishing. Halogen-free. Lower high-voltage values and insulation .. |