Thermal Properties Metric English Comments
Thermal Conductivity 125 - 140 W/m-K
868 - 972 BTU-in/hr-ft²-°F
Temper T651
Constellium ALPLAN® 2017A High-Strength Rolled Precision Aluminum Plate, Milled Both Sides
ALPLAN® 2017A precision plates combine a very good dimensional stability with a high level of mechanical strength and elongation. The outstanding flatness, the low roughness and high quality of the..
Thermal Conductivity 115 - 140 W/m-K
798 - 972 BTU-in/hr-ft²-°F
Temper T651
Constellium ALPLAN® 7075 High-Strength Rolled Precision Aluminum Plate, Milled Both Sides
ALPLAN® 7075 precision plates combine a good dimensional stability with high mechanical strength. Both the outstanding flatness and the low roughness of the surfaces, protected by a plastic film, m..
Thermal Conductivity 130 - 140 W/m-K
902 - 972 BTU-in/hr-ft²-°F
Constellium PLAN 5754 Aluminum Rolled Plate
Rolled plates in 5754 PLAN are optimized for minimum residual stress and improved dimensional tolerances. 5754 PLAN is mainly used for low stressed mechanical components, manufactured by intensive m..
Thermal Conductivity 130 - 140 W/m-K
902 - 972 BTU-in/hr-ft²-°F
Constellium PLAN OX 5754 Aluminum Rolled Plate
Rolled plates in 5754 PLAN OX are optimized for minimum residual stress, improved dimensional tolerances and for decorative* anodizing. 5754 PLAN OX is mainly used for low stressed, anodized compone..
Thermal Conductivity 109 - 140 W/m-K
756 - 972 BTU-in/hr-ft²-°F
ALIMEX ACP 5080 Aluminum Cast Plate
ACP 5080 is a 5xxx series precision aluminum cast plate. Thickness, flatness and surface finish offer very tight tolerances.Material stability and excellent processing characteristics make this alum..
Thermal Conductivity 109 - 140 W/m-K
756 - 972 BTU-in/hr-ft²-°F
ALIMEX ACP 5080R Aluminum Cast Material