Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 1.33 W/m-K | 9.23 BTU-in/hr-ft²-°F | |
Loctite® Output™ 5404 Heat Cure Silicone Thermally Conductive BondersLoctite® Thermally Conductive Adhesives eliminate the need for mechanical fasteners and clips, while providing the most efficient thermal transfer between transistors or.. |
|||
Thermal Conductivity | 1.33 W/m-K | 9.23 BTU-in/hr-ft²-°F | Product Property; ASTM E 1530 |
Arlon Thermabond® T20 (99710W015) 0.015" (0.381 mm) Uncured Silicone Rubber with PTFE Coated Fiberglass Carrier Description: 15 mil thick Thermabond® T20 electrically insulating electronic adhesive.Design/Construction: Liner: FEP Product: Uncured Silicone Rubber Carrier: PTFE Coated FiberglassRecommended Pri.. |