Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 121 W/m-K | 840 BTU-in/hr-ft²-°F | |
Eagle Brass 260 Cartridge Brass, 1/2 Hard Alloy C260 is commonly used for electrical components, electronic parts, and mechanical fasteners. The alloy has good strength but poor stress relaxation characteristics and does not make a particul.. |
|||
Thermal Conductivity | 121 W/m-K | 840 BTU-in/hr-ft²-°F | |
Eagle Brass 260 Cartridge Brass, 1/4 Hard Alloy C260 is commonly used for electrical components, electronic parts, and mechanical fasteners. The alloy has good strength but poor stress relaxation characteristics and does not make a particul.. |
|||
Thermal Conductivity | 121 W/m-K | 840 BTU-in/hr-ft²-°F | |
Eagle Brass 260 Cartridge Brass, 3/4 Hard Alloy C260 is commonly used for electrical components, electronic parts, and mechanical fasteners. The alloy has good strength but poor stress relaxation characteristics and does not make a particul.. |
|||
Thermal Conductivity | 121 W/m-K | 840 BTU-in/hr-ft²-°F | |
Eagle Brass 260 Cartridge Brass, Annealed Alloy C260 is commonly used for electrical components, electronic parts, and mechanical fasteners. The alloy has good strength but poor stress relaxation characteristics and does not make a particul.. |
|||
Thermal Conductivity | 121 W/m-K | 840 BTU-in/hr-ft²-°F | |
Eagle Brass 260 Cartridge Brass, Extra Hard Alloy C260 is commonly used for electrical components, electronic parts, and mechanical fasteners. The alloy has good strength but poor stress relaxation characteristics and does not make a particul.. |
|||
Thermal Conductivity | 121 W/m-K | 840 BTU-in/hr-ft²-°F | |
Eagle Brass 260 Cartridge Brass, Extra Spring Alloy C260 is commonly used for electrical components, electronic parts, and mechanical fasteners. The alloy has good strength but poor stress relaxation characteristics and does not make a particul.. |
|||
Thermal Conductivity | 121 W/m-K | 840 BTU-in/hr-ft²-°F | |
Eagle Brass 260 Cartridge Brass, Hard Alloy C260 is commonly used for electrical components, electronic parts, and mechanical fasteners. The alloy has good strength but poor stress relaxation characteristics and does not make a particul.. |
|||
Thermal Conductivity | 121 W/m-K | 840 BTU-in/hr-ft²-°F | |
Eagle Brass 260 Cartridge Brass, Spring Alloy C260 is commonly used for electrical components, electronic parts, and mechanical fasteners. The alloy has good strength but poor stress relaxation characteristics and does not make a particul.. |
|||
Thermal Conductivity | 121 W/m-K | 840 BTU-in/hr-ft²-°F | |
Chicago Extruded Metals BioBrass® UNS C26000 Copper-Zinc Alloy Finished product available as bar, wire, rod or tube.Chicago Extruded Metal temper codes: H01, H02, H04This alloy is registered with the U.S. EPA as Antimicrobial.Information provided by Chicago Ext.. |