Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 84.0 W/m-K | 583 BTU-in/hr-ft²-°F | |
Hogen HM1150 Tungsten-Based Metal Mil Spec T-21014D Class 2; AMS T-21014 Class 2; ASTM B-777-99 Class 2. Slightly Magnetic.Manufactured by powder metallurgy methods. The tungsten base offers high thermal conductivity and a low CTE.. |
|||
Thermal Conductivity | 84.0 W/m-K | 583 BTU-in/hr-ft²-°F | |
Mi-Tech Metals HD17.5 Tungsten-Based Metal Mil Spec T-21014D Class 2; AMS T-21014 Class 2; ASTM B-777-99 Class 2; ASTM B-777-07 Class 2. Slightly Magnetic.Manufactured by powder metallurgy methods. The tungsten base offers high thermal con.. |
|||
Thermal Conductivity | 84.0 W/m-K | 583 BTU-in/hr-ft²-°F | solid solution (or quenched) state |
CLAL-MSX SICLANIC S® TB Quenched Copper Alloy SICLANIC S® is particularly recommended for the production of conductive contact blades. SICLANIC S® offers :electrical conductivity greatly superior to that of bronzes, brasses and nickel silver.. |
|||
Thermal Conductivity | 84.0 W/m-K | 583 BTU-in/hr-ft²-°F | solid solution (or quenched) state |
CLAL-MSX SICLANIC S® TD4 Quenched Copper Alloy, 4/4 Hard SICLANIC S® is particularly recommended for the production of conductive contact blades. SICLANIC S® offers :electrical conductivity greatly superior to that of bronzes, brasses and nickel silver.. |
|||
Thermal Conductivity | 84.0 W/m-K | 583 BTU-in/hr-ft²-°F | solid solution (or quenched) state |
CLAL-MSX SICLANIC S® TF Quenched Copper Alloy, precipitation treated SICLANIC S® is particularly recommended for the production of conductive contact blades. SICLANIC S® offers :electrical conductivity greatly superior to that of bronzes, brasses and nickel silver.. |
|||
Thermal Conductivity | 84.0 W/m-K | 583 BTU-in/hr-ft²-°F | solid solution (or quenched) state |
CLAL-MSX SICLANIC S® TH3 Quenched Copper Alloy, 1/2 Hard, precipitation treated SICLANIC S® is particularly recommended for the production of conductive contact blades. SICLANIC S® offers :electrical conductivity greatly superior to that of bronzes, brasses and nickel silver.. |
|||
Thermal Conductivity | 84.0 W/m-K | 583 BTU-in/hr-ft²-°F | solid solution (or quenched) state |
CLAL-MSX SICLANIC S® TH4 Quenched Copper Alloy, 4/4 Hard, precipitation treated SICLANIC S® is particularly recommended for the production of conductive contact blades. SICLANIC S® offers :electrical conductivity greatly superior to that of bronzes, brasses and nickel silver.. |
|||
Thermal Conductivity | 84.0 W/m-K | 583 BTU-in/hr-ft²-°F | solid solution (or quenched) state |
CLAL-MSX SICLANIC S® TD3 Quenched Copper Alloy, 1/2 Hard SICLANIC S® is particularly recommended for the production of conductive contact blades. SICLANIC S® offers :electrical conductivity greatly superior to that of bronzes, brasses and nickel silver.. |