Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Thermal Conductivity = 79.8 BTU-in/hr-ft²-°F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Thermal Conductivity 11.5 W/m-K
79.8 BTU-in/hr-ft²-°F
RT
Haynes Hastelloy® N, 1.14 mm sheet, aged 10000 hours at 538°C (1000°F)
Applications include containers for molten fluoride salts. Good oxidation resistance to hot fluoride salts at 705-870°C (1300-1600°F), good oxidation resistance in air.Data provided by the man..
Thermal Conductivity 11.5 W/m-K
79.8 BTU-in/hr-ft²-°F
RT
Haynes Hastelloy® N, 1.14 mm sheet, aged 10000 hours at 704°C (1300°F)
Applications include containers for molten fluoride salts. Good oxidation resistance to hot fluoride salts at 705-870°C (1300-1600°F), good oxidation resistance in air.Data provided by the man..
Thermal Conductivity 11.5 W/m-K
79.8 BTU-in/hr-ft²-°F
RT
Haynes Hastelloy® N, 1.6 mm sheet, heat treated at 1175°C, welded and tested as welded
Applications include containers for molten fluoride salts. Good oxidation resistance to hot fluoride salts at 705-870°C (1300-1600°F), good oxidation resistance in air.Data provided by the man..
Thermal Conductivity 11.5 W/m-K
79.8 BTU-in/hr-ft²-°F
RT
Haynes Hastelloy® N, weld metal as welded
Applications include containers for molten fluoride salts. Good oxidation resistance to hot fluoride salts at 705-870°C (1300-1600°F), good oxidation resistance in air.Data provided by the man..
Thermal Conductivity 11.5 W/m-K
79.8 BTU-in/hr-ft²-°F
RT
Haynes Hastelloy® N, weld metal, aged 500 hours at 649°C (1200°F)
Applications include containers for molten fluoride salts. Good oxidation resistance to hot fluoride salts at 705-870°C (1300-1600°F), good oxidation resistance in air.Data provided by the man..
Thermal Conductivity 11.5 W/m-K
79.8 BTU-in/hr-ft²-°F
Special Metals INCOLOY® 25-6M0 Super Austenitic Stainless Steel (UNS N08926)
Data provided by the manufacturer, Special Metals.
Thermal Conductivity 11.5 W/m-K
79.8 BTU-in/hr-ft²-°F
Special Metals INCOLOY® Alloy 800
A nickel-iron-chromium alloy with good strength and excellent resistance to oxidation and carburization in high-temperature atmospheres. It also resists corrosion by many aqueous environments. The..
Thermal Conductivity 11.5 W/m-K
79.8 BTU-in/hr-ft²-°F
Special Metals INCOLOY® Alloy 800HT™
A nickel-iron-chromium alloy having the same basic composition as INCOLOY alloy 800 but with significantly higher creep-rupture strength. The higher strength results from close control of the carbo..
Thermal Conductivity 11.5 W/m-K
79.8 BTU-in/hr-ft²-°F
Special Metals NIMONIC® Alloy 90
A precipitation-hardenable nickel-chromium-cobalt alloy having high stress-rupture strength and creep resistance at temperatures to about 1700°F (920°C). The alloy also has good resistance to..
Thermal Conductivity 11.5 W/m-K
79.8 BTU-in/hr-ft²-°F
RT
Haynes Hastelloy® N, 1.14 mm sheet, aged 10000 hours at 593°C (1100°F)
Applications include containers for molten fluoride salts. Good oxidation resistance to hot fluoride salts at 705-870°C (1300-1600°F), good oxidation resistance in air.Data provided by the manufac..
Thermal Conductivity 11.5 W/m-K
79.8 BTU-in/hr-ft²-°F
RT
Haynes Hastelloy® N, 1.14 mm sheet, aged 10000 hours at 760°C (1400°F)
Applications include containers for molten fluoride salts. Good oxidation resistance to hot fluoride salts at 705-870°C (1300-1600°F), good oxidation resistance in air.Data provided by the manufac..
Thermal Conductivity 11.5 W/m-K
79.8 BTU-in/hr-ft²-°F
RT
Haynes Hastelloy® N, 1.6 mm sheet, aged 128 hours at 815°C (1500°F)
Applications include containers for molten fluoride salts. Good oxidation resistance to hot fluoride salts at 705-870°C (1300-1600°F), good oxidation resistance in air.Data provided by the manufac..
Thermal Conductivity 11.5 W/m-K
79.8 BTU-in/hr-ft²-°F
RT
Haynes Hastelloy® N, 1.6 mm sheet, heat treated at 1175°C, rapid air cooled
Applications include containers for molten fluoride salts. Good oxidation resistance to hot fluoride salts at 705-870°C (1300-1600°F), good oxidation resistance in air.Data provided by the manufac..
Thermal Conductivity 11.5 W/m-K
79.8 BTU-in/hr-ft²-°F
RT
Haynes Hastelloy® N, 1.14 mm sheet, aged 10000 hours at 649°C (1200°F)
Applications include containers for molten fluoride salts. Good oxidation resistance to hot fluoride salts at 705-870°C (1300-1600°F), good oxidation resistance in air.Data provided by the manufac..
Thermal Conductivity 11.5 W/m-K
79.8 BTU-in/hr-ft²-°F
RT
Haynes Hastelloy® N, 1.14 mm sheet, heat treated at 1149°C (2100°F)
Applications include containers for molten fluoride salts. Good oxidation resistance to hot fluoride salts at 705-870°C (1300-1600°F), good oxidation resistance in air.Data provided by the manufac..
Copyright © lookpolymers.com All Rights Reserved