Polymer Property : Thermal Conductivity = 583 BTU-in/hr-ft²-°F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Thermal Conductivity 84.0 W/m-K
583 BTU-in/hr-ft²-°F
Hogen HM1150 Tungsten-Based Metal
Mil Spec T-21014D Class 2; AMS T-21014 Class 2; ASTM B-777-99 Class 2. Slightly Magnetic.Manufactured by powder metallurgy methods. The tungsten base offers high thermal conductivity and a low CTE..
Thermal Conductivity 84.0 W/m-K
583 BTU-in/hr-ft²-°F
Mi-Tech Metals HD17.5 Tungsten-Based Metal
Mil Spec T-21014D Class 2; AMS T-21014 Class 2; ASTM B-777-99 Class 2; ASTM B-777-07 Class 2. Slightly Magnetic.Manufactured by powder metallurgy methods. The tungsten base offers high thermal con..
Thermal Conductivity 84.0 W/m-K
583 BTU-in/hr-ft²-°F
solid solution (or quenched) state
CLAL-MSX SICLANIC S® TB Quenched Copper Alloy
SICLANIC S® is particularly recommended for the production of conductive contact blades. SICLANIC S® offers :electrical conductivity greatly superior to that of bronzes, brasses and nickel silver..
Thermal Conductivity 84.0 W/m-K
583 BTU-in/hr-ft²-°F
solid solution (or quenched) state
CLAL-MSX SICLANIC S® TD4 Quenched Copper Alloy, 4/4 Hard
SICLANIC S® is particularly recommended for the production of conductive contact blades. SICLANIC S® offers :electrical conductivity greatly superior to that of bronzes, brasses and nickel silver..
Thermal Conductivity 84.0 W/m-K
583 BTU-in/hr-ft²-°F
solid solution (or quenched) state
CLAL-MSX SICLANIC S® TF Quenched Copper Alloy, precipitation treated
SICLANIC S® is particularly recommended for the production of conductive contact blades. SICLANIC S® offers :electrical conductivity greatly superior to that of bronzes, brasses and nickel silver..
Thermal Conductivity 84.0 W/m-K
583 BTU-in/hr-ft²-°F
solid solution (or quenched) state
CLAL-MSX SICLANIC S® TH3 Quenched Copper Alloy, 1/2 Hard, precipitation treated
SICLANIC S® is particularly recommended for the production of conductive contact blades. SICLANIC S® offers :electrical conductivity greatly superior to that of bronzes, brasses and nickel silver..
Thermal Conductivity 84.0 W/m-K
583 BTU-in/hr-ft²-°F
solid solution (or quenched) state
CLAL-MSX SICLANIC S® TH4 Quenched Copper Alloy, 4/4 Hard, precipitation treated
SICLANIC S® is particularly recommended for the production of conductive contact blades. SICLANIC S® offers :electrical conductivity greatly superior to that of bronzes, brasses and nickel silver..
Thermal Conductivity 84.0 W/m-K
583 BTU-in/hr-ft²-°F
solid solution (or quenched) state
CLAL-MSX SICLANIC S® TD3 Quenched Copper Alloy, 1/2 Hard
SICLANIC S® is particularly recommended for the production of conductive contact blades. SICLANIC S® offers :electrical conductivity greatly superior to that of bronzes, brasses and nickel silver..