Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 0.711 - 0.837 W/m-K | 4.93 - 5.80 BTU-in/hr-ft²-°F | |
Polikim EFALON® B-40 PTFE, 40% Bronze Filled Bronze-filled Efalon® (PTFE) has better heat insulation, less thermal expansion, higher wear resistance properties and less deformation under load compared to virgin Efalon®. Applications: bearing.. |
|||
Thermal Conductivity | 0.711 - 0.837 W/m-K | 4.93 - 5.80 BTU-in/hr-ft²-°F | |
Polikim EFALON® B-60 PTFE, 60% Bronze Filled Bronze-filled Efalon® (PTFE) has better heat insulation, less thermal expansion, higher wear resistance properties and less deformation under load compared to virgin Efalon®. Applications: bearing.. |