Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 18.5 - 43.7 W/m-K @Temperature 85.0 - 85.0 °C |
128 - 303 BTU-in/hr-ft²-°F @Temperature 185 - 185 °F |
Average value: 31.1 W/m-K Grade Count:1 |
Overview of materials for Vinyl Ester Sheet Molding Compound This property data is a summary of similar materials in the MatWeb database for the category "Vinyl Ester Sheet Molding Compound". Each property range of values reported is minimum and maximum value.. |