Thermal Properties Metric English Comments
Thermal Conductivity 390.8 W/m-K
2712 BTU-in/hr-ft²-°F
Eagle Brass 110 EPT COPPER, 1/2 Hard
Alloy 110, also known as electrolytic tough pitch (ETP) copper, is commonly used in electric current carrying applications. 110 Copper is 99.9% pure copper with an electrical conductivity rating of ..
Thermal Conductivity 390.8 W/m-K
2712 BTU-in/hr-ft²-°F
Eagle Brass 110 EPT COPPER, 1/4 Hard
Alloy 110, also known as electrolytic tough pitch (ETP) copper, is commonly used in electric current carrying applications. 110 Copper is 99.9% pure copper with an electrical conductivity rating of ..
Thermal Conductivity 390.8 W/m-K
2712 BTU-in/hr-ft²-°F
Eagle Brass 110 EPT COPPER, 3/4 Hard
Alloy 110, also known as electrolytic tough pitch (ETP) copper, is commonly used in electric current carrying applications. 110 Copper is 99.9% pure copper with an electrical conductivity rating of ..
Thermal Conductivity 390.8 W/m-K
2712 BTU-in/hr-ft²-°F
Eagle Brass 110 EPT COPPER, Annealed
Alloy 110, also known as electrolytic tough pitch (ETP) copper, is commonly used in electric current carrying applications. 110 Copper is 99.9% pure copper with an electrical conductivity rating of ..
Thermal Conductivity 390.8 W/m-K
2712 BTU-in/hr-ft²-°F
Eagle Brass 110 EPT COPPER, Extra Hard
Alloy 110, also known as electrolytic tough pitch (ETP) copper, is commonly used in electric current carrying applications. 110 Copper is 99.9% pure copper with an electrical conductivity rating of ..
Thermal Conductivity 390.8 W/m-K
2712 BTU-in/hr-ft²-°F
Eagle Brass 110 EPT COPPER, Extra Spring
Alloy 110, also known as electrolytic tough pitch (ETP) copper, is commonly used in electric current carrying applications. 110 Copper is 99.9% pure copper with an electrical conductivity rating of ..
Thermal Conductivity 390.8 W/m-K
2712 BTU-in/hr-ft²-°F
Eagle Brass 110 EPT COPPER, Hard
Alloy 110, also known as electrolytic tough pitch (ETP) copper, is commonly used in electric current carrying applications. 110 Copper is 99.9% pure copper with an electrical conductivity rating of ..
Thermal Conductivity 390.8 W/m-K
2712 BTU-in/hr-ft²-°F
Eagle Brass 110 EPT COPPER, Spring
Alloy 110, also known as electrolytic tough pitch (ETP) copper, is commonly used in electric current carrying applications. 110 Copper is 99.9% pure copper with an electrical conductivity rating of ..
Thermal Conductivity 390.8 W/m-K
2712 BTU-in/hr-ft²-°F
Eagle Brass 101 OFE COPPER (Certified), 1/2 Hard
Alloy 101 is known as Oxygen-Free Electronic (OFE). It reaches a minimum of 101% IACS conductivity rating. It is the most expensive out of the 101- 110 group because of its higher purity.Information..
Thermal Conductivity 390.8 W/m-K
2712 BTU-in/hr-ft²-°F
Eagle Brass 101 OFE COPPER (Certified), 3/4 Hard
Alloy 101 is known as Oxygen-Free Electronic (OFE). It reaches a minimum of 101% IACS conductivity rating. It is the most expensive out of the 101- 110 group because of its higher purity.Information..
Thermal Conductivity 390.8 W/m-K
2712 BTU-in/hr-ft²-°F
Eagle Brass 101 OFE COPPER (Certified), Annealed
Alloy 101 is known as Oxygen-Free Electronic (OFE). It reaches a minimum of 101% IACS conductivity rating. It is the most expensive out of the 101- 110 group because of its higher purity.Information..
Thermal Conductivity 390.8 W/m-K
2712 BTU-in/hr-ft²-°F
Eagle Brass 101 OFE COPPER (Certified), Extra Hard
Alloy 101 is known as Oxygen-Free Electronic (OFE). It reaches a minimum of 101% IACS conductivity rating. It is the most expensive out of the 101- 110 group because of its higher purity.Information..
Thermal Conductivity 390.8 W/m-K
2712 BTU-in/hr-ft²-°F
Eagle Brass 101 OFE COPPER (Certified), Extra Spring
Alloy 101 is known as Oxygen-Free Electronic (OFE). It reaches a minimum of 101% IACS conductivity rating. It is the most expensive out of the 101- 110 group because of its higher purity.Information..
Thermal Conductivity 390.8 W/m-K
2712 BTU-in/hr-ft²-°F
Eagle Brass 101 OFE COPPER (Certified), Hard
Alloy 101 is known as Oxygen-Free Electronic (OFE). It reaches a minimum of 101% IACS conductivity rating. It is the most expensive out of the 101- 110 group because of its higher purity.Information..
Thermal Conductivity 390.8 W/m-K
2712 BTU-in/hr-ft²-°F
Eagle Brass 101 OFE COPPER (Certified), Spring
Alloy 101 is known as Oxygen-Free Electronic (OFE). It reaches a minimum of 101% IACS conductivity rating. It is the most expensive out of the 101- 110 group because of its higher purity.Information..
Thermal Conductivity 390.8 W/m-K
2712 BTU-in/hr-ft²-°F
Eagle Brass 102 OF COPPER (Non-Certified), 1/2 Hard
Alloy 102 is an oxygen-free copper which has better forming, resistance to hydrogen embrittlement, and brazing characteristics than C110 ETP. C102 has good solder-ability and corrosion resistance an..
Thermal Conductivity 390.8 W/m-K
2712 BTU-in/hr-ft²-°F
Eagle Brass 102 OF COPPER (Non-Certified), 1/4 Hard
Alloy 102 is an oxygen-free copper which has better forming, resistance to hydrogen embrittlement, and brazing characteristics than C110 ETP. C102 has good solder-ability and corrosion resistance an..
Thermal Conductivity 390.8 W/m-K
2712 BTU-in/hr-ft²-°F
Eagle Brass 102 OF COPPER (Non-Certified), 3/4 Hard
Alloy 102 is an oxygen-free copper which has better forming, resistance to hydrogen embrittlement, and brazing characteristics than C110 ETP. C102 has good solder-ability and corrosion resistance an..
Thermal Conductivity 390.8 W/m-K
2712 BTU-in/hr-ft²-°F
Eagle Brass 102 OF COPPER (Non-Certified), Annealed
Alloy 102 is an oxygen-free copper which has better forming, resistance to hydrogen embrittlement, and brazing characteristics than C110 ETP. C102 has good solder-ability and corrosion resistance an..
Thermal Conductivity 390.8 W/m-K
2712 BTU-in/hr-ft²-°F
Eagle Brass 102 OF COPPER (Non-Certified), Extra Hard
Alloy 102 is an oxygen-free copper which has better forming, resistance to hydrogen embrittlement, and brazing characteristics than C110 ETP. C102 has good solder-ability and corrosion resistance an..
Thermal Conductivity 390.8 W/m-K
2712 BTU-in/hr-ft²-°F
Eagle Brass 102 OF COPPER (Non-Certified), Extra Spring
Alloy 102 is an oxygen-free copper which has better forming, resistance to hydrogen embrittlement, and brazing characteristics than C110 ETP. C102 has good solder-ability and corrosion resistance an..
Thermal Conductivity 390.8 W/m-K
2712 BTU-in/hr-ft²-°F
Eagle Brass 102 OF COPPER (Non-Certified), Hard
Alloy 102 is an oxygen-free copper which has better forming, resistance to hydrogen embrittlement, and brazing characteristics than C110 ETP. C102 has good solder-ability and corrosion resistance an..
Thermal Conductivity 390.8 W/m-K
2712 BTU-in/hr-ft²-°F
Eagle Brass 102 OF COPPER (Non-Certified), Spring
Alloy 102 is an oxygen-free copper which has better forming, resistance to hydrogen embrittlement, and brazing characteristics than C110 ETP. C102 has good solder-ability and corrosion resistance an..
Thermal Conductivity 390.8 W/m-K
2712 BTU-in/hr-ft²-°F
Eagle Brass 101 OFE COPPER (Certified), 1/4 Hard
Alloy 101 is known as Oxygen-Free Electronic (OFE). It reaches a minimum of 101% IACS conductivity rating. It is the most expensive out of the 101- 110 group because of its higher purity.Information..