Polymer Property : Thermal Conductivity = 303 BTU-in/hr-ft²-°F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Thermal Conductivity 18.5 - 43.7 W/m-K

@Temperature 85.0 - 85.0 °C
128 - 303 BTU-in/hr-ft²-°F

@Temperature 185 - 185 °F
Average value: 31.1 W/m-K Grade Count:1
Overview of materials for Vinyl Ester Sheet Molding Compound
This property data is a summary of similar materials in the MatWeb database for the category "Vinyl Ester Sheet Molding Compound". Each property range of values reported is minimum and maximum value..