Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 0.480 W/m-K @Temperature 80.0 °C |
3.33 BTU-in/hr-ft²-°F @Temperature 176 °F |
ASTM C518 |
Rogers Corporation RO3203 Woven-Glass Reinforced PTFE Laminate Features and Benefits:Woven glass reinforcement - Improves rigidity for easier handlingUniform electrical and mechanical performance - ideal for complex multi-layer high frequency structuresLow diel.. |
|||
Thermal Conductivity | 0.480 W/m-K | 3.33 BTU-in/hr-ft²-°F | |
Premix Premi-Glas® 1268 Fiberglass Reinforced Thermoset Thick Molding Compound Premi-Glas® 1268 is a fiberglass reinforced thermoset thick molding compound for composite power train applications such as valve covers and timing gear covers.Key features and benefits are:Ideal f.. |
|||
Thermal Conductivity | 0.480 W/m-K | 3.33 BTU-in/hr-ft²-°F | DIN 52612 |
Lehmann & Voss LUVOCOM® 20-0659 Polyphthalamide, with carbon fiber Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Low influence from moisture an.. |
|||
Thermal Conductivity | 0.480 W/m-K | 3.33 BTU-in/hr-ft²-°F | DIN 52612 |
Lehmann & Voss LUVOCOM® 204-8468 Polyphthalamide, with carbon fiber Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Low influence from moisture an.. |
|||
Thermal Conductivity | 0.480 W/m-K | 3.33 BTU-in/hr-ft²-°F | ASTM D177 |
Iran Petrochemical (PCC) 3840 UA Medium Density Polyethylene MD3840UA is a linear medium density polyethylene (MDPE) with butene copolymer. This polymer has good impact strength, excellent external and internal surface finish, whiteness, good stress cracking .. |
|||
Thermal Conductivity | 0.480 W/m-K | 3.33 BTU-in/hr-ft²-°F | ASTM D177 |
Iran Petrochemical (PCC) 6070EA High Density Polyethylene HD6070EA is a high density polyethylene with a narrow molecular weight distribution. It is suitable for a wide range of injection molding applications. This grade has following characteristics: easy.. |
|||
Thermal Conductivity | 0.480 W/m-K @Temperature 100 °C |
3.33 BTU-in/hr-ft²-°F @Temperature 212 °F |
ASTM E1461 |
Plenco 4301 Phenolic, Granular, Compression Molded PLENCO 04301 is a heat resistant, mineral filled phenolic molding compound offering excellent dimensional stability and electrical properties. UL recognized under component file E40654. 04301 is ava.. |
|||
Thermal Conductivity | 0.480 W/m-K | 3.33 BTU-in/hr-ft²-°F | ASTM E1461 |
Vyncolit BXE7665 Glass Filled Phenolic Molding Compound Novolac resin based, mainly glass fiber filled. Excellent electrical properties combined with very good mechanical properties. Grade especially suitable for electrical applications.Information pro.. |