Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 0.170 - 0.330 W/m-K | 1.18 - 2.29 BTU-in/hr-ft²-°F | ASTM C177 |
Eastman Tenite 105E3V36327 Acetate Clear, Trsp Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a warm feel. The mechanical properties if Tenite cellulosi.. |
|||
Thermal Conductivity | 0.170 - 0.330 W/m-K | 1.18 - 2.29 BTU-in/hr-ft²-°F | ASTM C177 |
Eastman Tenite 285E0V16304 Cellulose Acetate Butyrate, Clear, Trsp Applications:DisplaysProduct Description: Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a warm feel. T.. |
|||
Thermal Conductivity | 0.170 - 0.330 W/m-K | 1.18 - 2.29 BTU-in/hr-ft²-°F | ASTM C177 |
Eastman Tenite 285E3720005 Butyrate Clear, Trsp Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a warm feel. The mechanical properties of Tenite cellulosi.. |
|||
Thermal Conductivity | 0.170 - 0.330 W/m-K | 1.18 - 2.29 BTU-in/hr-ft²-°F | ASTM C177 |
Eastman Tenite 307A4000015 Propionate Clear, Trsp Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a warm feel. The mechanical properties if Tenite cellulosi.. |
|||
Thermal Conductivity | 0.170 - 0.330 W/m-K | 1.18 - 2.29 BTU-in/hr-ft²-°F | ASTM C177 |
Eastman Tenite 307E4000018 Propionate Clear, Trsp Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a warm feel. The mechanical properties if Tenite cellulosi.. |
|||
Thermal Conductivity | 0.170 - 0.330 W/m-K | 1.18 - 2.29 BTU-in/hr-ft²-°F | ASTM C177 |
Eastman Tenite 350A0096914 Propionate Natural Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a warm feel. The mechanical properties of Tenite cellulosi.. |
|||
Thermal Conductivity | 0.170 - 0.330 W/m-K | 1.18 - 2.29 BTU-in/hr-ft²-°F | ASTM C177 |
Eastman Tenite 350A4861313 Cellulose Acetate Propionate, Clear, Trsp Applications:Blood TherapyDrug DeliveryIV ComponentsMedical DevicesSurgical InstrumentsProduct Description: Tenite cellulosic plastics are noted for their excellent balance of properties - toughne.. |
|||
Thermal Conductivity | 0.170 - 0.330 W/m-K | 1.18 - 2.29 BTU-in/hr-ft²-°F | ASTM C177 |
Eastman Tenite 360A4000012 Propionate Clear, Trsp Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a warm feel. The mechanical properties if Tenite cellulosi.. |
|||
Thermal Conductivity | 0.170 - 0.330 W/m-K | 1.18 - 2.29 BTU-in/hr-ft²-°F | ASTM C177 |
Eastman Tenite 360A4861307 Cellulose Acetate Propionate, Clear, Trsp Applications:Blood TherapyDrug DeliveryIV ComponentsMedical DevicesSurgical InstrumentsKey Attributes:Chemical resistance to most medical solvents including lipids and IPAEase of processingGamma and.. |
|||
Thermal Conductivity | 0.170 - 0.330 W/m-K | 1.18 - 2.29 BTU-in/hr-ft²-°F | ASTM C177 |
Eastman Tenite 360A4861316 Propionate Clear, Trsp Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a warm feel. The mechanical properties if Tenite cellulosi.. |
|||
Thermal Conductivity | 0.170 - 0.330 W/m-K | 1.18 - 2.29 BTU-in/hr-ft²-°F | ASTM C177 |
Eastman Tenite 360E0096914 Cellulose Acetate Propionate, Natural, Trsp Applications:ProfilesProduct Description: Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a warm feel. T.. |
|||
Thermal Conductivity | 0.170 - 0.330 W/m-K | 1.18 - 2.29 BTU-in/hr-ft²-°F | ASTM C177 |
Eastman Tenite 360E2R30016 Cellulose Acetate Propionate, Natural, Trsp Applications:AppliancesPersonal Care and CosmeticsProduct Description: Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss.. |
|||
Thermal Conductivity | 0.170 - 0.330 W/m-K | 1.18 - 2.29 BTU-in/hr-ft²-°F | ASTM C177 |
Eastman Tenite 360E3V45508 Propionate Water Clear, Trsp Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a warm feel. The mechanical properties of Tenite cellulosi.. |
|||
Thermal Conductivity | 0.170 - 0.330 W/m-K | 1.18 - 2.29 BTU-in/hr-ft²-°F | ASTM C177 |
Eastman Tenite 360E3V45516 Propionate Water Clear, Trsp Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a warm feel. The mechanical properties of Tenite cellulosi.. |
|||
Thermal Conductivity | 0.170 - 0.330 W/m-K | 1.18 - 2.29 BTU-in/hr-ft²-°F | ASTM C177 |
Eastman Tenite 360E461312 Propionate Clear, Trsp Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a warm feel. The mechanical properties of Tenite cellulosi.. |
|||
Thermal Conductivity | 0.170 - 0.330 W/m-K | 1.18 - 2.29 BTU-in/hr-ft²-°F | ASTM C177 |
Eastman Tenite 360E4861314 Cellulose Acetate Propionate, Clear, Trsp Applications:ProfilesProduct Description: Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a warm feel. T.. |
|||
Thermal Conductivity | 0.170 - 0.330 W/m-K | 1.18 - 2.29 BTU-in/hr-ft²-°F | ASTM C177 |
Eastman Tenite 360E4861316 Cellulose Acetate Propionate, Clear, Trsp Applications:ProfilesProduct Description: Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a warm feel. T.. |
|||
Thermal Conductivity | 0.170 - 0.330 W/m-K | 1.18 - 2.29 BTU-in/hr-ft²-°F | ASTM C177 |
Eastman Tenite 371A2R30008 Cellulose Acetate Propionate, Natural, Trsp Applications:Consumer-Personal CareToothbrushesProduct Description: Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, c.. |
|||
Thermal Conductivity | 0.170 - 0.330 W/m-K | 1.18 - 2.29 BTU-in/hr-ft²-°F | ASTM C177 |
Eastman Tenite 371A4000012 Cellulose Acetate Propionate, Clear, Trsp Applications:OphthalmicsOral HygienePen/stationary suppliesToothbrushesProduct Description: Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, st.. |
|||
Thermal Conductivity | 0.170 - 0.330 W/m-K | 1.18 - 2.29 BTU-in/hr-ft²-°F | ASTM C177 |
Eastman Tenite 380A4000015 Cellulose Acetate Propionate, Clear, Trsp Applications:OphthalmicsProduct Description: Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a warm feel.. |
|||
Thermal Conductivity | 0.170 - 0.330 W/m-K | 1.18 - 2.29 BTU-in/hr-ft²-°F | ASTM C177 |
Eastman Tenite 383A2R30010 Cellulose Acetate Propionate, Natural, Trsp Applications:Oral HygienePlastics for hygiene feminine productsRecreationalToothbrushesProduct Description: Tenite cellulosic plastics are noted for their excellent balance of properties - toughne.. |
|||
Thermal Conductivity | 0.170 - 0.330 W/m-K | 1.18 - 2.29 BTU-in/hr-ft²-°F | ASTM C177 |
Eastman Tenite 383A4000011 Cellulose Acetate Propionate, Clear, Trsp Applications:AppliancesFloor carePersonal care and cosmeticsProfilesProduct Description: Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, stren.. |
|||
Thermal Conductivity | 0.170 - 0.330 W/m-K | 1.18 - 2.29 BTU-in/hr-ft²-°F | ASTM C177 |
Eastman Tenite 485E3720008 Cellulose Acetate Butyrate, Clear, Trsp Applications:Toys/Sporting goodsProduct Description: Tenite cellulosic plastics are noted for their excellent balance of properties including toughness, hardness, strength, surface gloss, clarity,.. |
|||
Thermal Conductivity | 0.170 - 0.330 W/m-K | 1.18 - 2.29 BTU-in/hr-ft²-°F | ASTM C177 |
Eastman Tenite 485E3720023 Butyrate Clear, Trsp Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a warm feel. The mechanical properties of Tenite cellulosi.. |
|||
Thermal Conductivity | 0.250 - 0.330 W/m-K | 1.74 - 2.29 BTU-in/hr-ft²-°F | Average value: 0.265 W/m-K Grade Count:13 |
Overview of materials for Nylon 6, Heat Stabilized This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Heat Stabilized". Each property range of values reported is minimum and maximum values of appro.. |
|||
Thermal Conductivity | 0.170 - 0.330 W/m-K | 1.18 - 2.29 BTU-in/hr-ft²-°F | Average value: 0.250 W/m-K Grade Count:45 |
Overview of materials for Cellulose Acetate Propionate, Molded This property data is a summary of similar materials in the MatWeb database for the category "Cellulose Acetate Propionate, Molded". Each property range of values reported is minimum and maximum val.. |
|||
Thermal Conductivity | 0.170 - 0.330 W/m-K | 1.18 - 2.29 BTU-in/hr-ft²-°F | Average value: 0.250 W/m-K Grade Count:5 |
Overview of materials for Cellulose Acetate, Molded This property data is a summary of similar materials in the MatWeb database for the category "Cellulose Acetate, Molded". Each property range of values reported is minimum and maximum values of appr.. |
|||
Thermal Conductivity | 0.170 - 0.330 W/m-K | 1.18 - 2.29 BTU-in/hr-ft²-°F | Average value: 0.250 W/m-K Grade Count:33 |
Overview of materials for Cellulose Acetate Butyrate, Molded This property data is a summary of similar materials in the MatWeb database for the category "Cellulose Acetate Butyrate, Molded". Each property range of values reported is minimum and maximum value.. |
|||
Thermal Conductivity | 0.170 - 0.330 W/m-K | 1.18 - 2.29 BTU-in/hr-ft²-°F | ASTM C177 |
Eastman Tenite 550E3V45510 Butyrate Water Clear, Trsp
(discontinued **) Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a warm feel. The mechanical properties of Tenite cellulosi.. |
|||
Thermal Conductivity | 0.170 - 0.330 W/m-K | 1.18 - 2.29 BTU-in/hr-ft²-°F | ASTM C177 |
Eastman Tenite 360A4861301 Propionate Clear, Trsp
(discontinued **) Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a warm feel. The mechanical properties if Tenite cellulosi.. |