Polymer Property : Thermal Conductivity = 188.5 W/m-K Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Thermal Conductivity 188.5 W/m-K
1308 BTU-in/hr-ft²-°F
Eagle Brass 220 Commercial Bronze, 1/2 Hard
CDA 220 is known for having very good corrosion resistance, great cold workability and good hot workability for drawing, blanking, coining, stamping, piercing and punching. Typical uses include plum..
Thermal Conductivity 188.5 W/m-K
1308 BTU-in/hr-ft²-°F
Eagle Brass 220 Commercial Bronze, 1/4 Hard
CDA 220 is known for having very good corrosion resistance, great cold workability and good hot workability for drawing, blanking, coining, stamping, piercing and punching. Typical uses include plum..
Thermal Conductivity 188.5 W/m-K
1308 BTU-in/hr-ft²-°F
Eagle Brass 220 Commercial Bronze, 3/4 Hard
CDA 220 is known for having very good corrosion resistance, great cold workability and good hot workability for drawing, blanking, coining, stamping, piercing and punching. Typical uses include plum..
Thermal Conductivity 188.5 W/m-K
1308 BTU-in/hr-ft²-°F
Eagle Brass 220 Commercial Bronze, Annealed
CDA 220 is known for having very good corrosion resistance, great cold workability and good hot workability for drawing, blanking, coining, stamping, piercing and punching. Typical uses include plum..
Thermal Conductivity 188.5 W/m-K
1308 BTU-in/hr-ft²-°F
Eagle Brass 220 Commercial Bronze, Extra Hard
CDA 220 is known for having very good corrosion resistance, great cold workability and good hot workability for drawing, blanking, coining, stamping, piercing and punching. Typical uses include plum..
Thermal Conductivity 188.5 W/m-K
1308 BTU-in/hr-ft²-°F
Eagle Brass 220 Commercial Bronze, Extra Spring
CDA 220 is known for having very good corrosion resistance, great cold workability and good hot workability for drawing, blanking, coining, stamping, piercing and punching. Typical uses include plum..
Thermal Conductivity 188.5 W/m-K
1308 BTU-in/hr-ft²-°F
Eagle Brass 220 Commercial Bronze, Hard
CDA 220 is known for having very good corrosion resistance, great cold workability and good hot workability for drawing, blanking, coining, stamping, piercing and punching. Typical uses include plum..
Thermal Conductivity 188.5 W/m-K
1308 BTU-in/hr-ft²-°F
Eagle Brass 220 Commercial Bronze, Spring
CDA 220 is known for having very good corrosion resistance, great cold workability and good hot workability for drawing, blanking, coining, stamping, piercing and punching. Typical uses include plum..
Thermal Conductivity 188.5 W/m-K
1308 BTU-in/hr-ft²-°F
Chicago Extruded Metals BioBrass® UNS C22000 Copper-Zinc Alloy
Finished product available as bar or wire.Chicago Extruded Metal temper codes: H01, H02, H04This alloy is registered with the U.S. EPA as Antimicrobial.Information provided by Chicago Extruded Metal..