Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 188.5 W/m-K | 1308 BTU-in/hr-ft²-°F | |
Eagle Brass 220 Commercial Bronze, 1/2 Hard CDA 220 is known for having very good corrosion resistance, great cold workability and good hot workability for drawing, blanking, coining, stamping, piercing and punching. Typical uses include plum.. |
|||
Thermal Conductivity | 188.5 W/m-K | 1308 BTU-in/hr-ft²-°F | |
Eagle Brass 220 Commercial Bronze, 1/4 Hard CDA 220 is known for having very good corrosion resistance, great cold workability and good hot workability for drawing, blanking, coining, stamping, piercing and punching. Typical uses include plum.. |
|||
Thermal Conductivity | 188.5 W/m-K | 1308 BTU-in/hr-ft²-°F | |
Eagle Brass 220 Commercial Bronze, 3/4 Hard CDA 220 is known for having very good corrosion resistance, great cold workability and good hot workability for drawing, blanking, coining, stamping, piercing and punching. Typical uses include plum.. |
|||
Thermal Conductivity | 188.5 W/m-K | 1308 BTU-in/hr-ft²-°F | |
Eagle Brass 220 Commercial Bronze, Annealed CDA 220 is known for having very good corrosion resistance, great cold workability and good hot workability for drawing, blanking, coining, stamping, piercing and punching. Typical uses include plum.. |
|||
Thermal Conductivity | 188.5 W/m-K | 1308 BTU-in/hr-ft²-°F | |
Eagle Brass 220 Commercial Bronze, Extra Hard CDA 220 is known for having very good corrosion resistance, great cold workability and good hot workability for drawing, blanking, coining, stamping, piercing and punching. Typical uses include plum.. |
|||
Thermal Conductivity | 188.5 W/m-K | 1308 BTU-in/hr-ft²-°F | |
Eagle Brass 220 Commercial Bronze, Extra Spring CDA 220 is known for having very good corrosion resistance, great cold workability and good hot workability for drawing, blanking, coining, stamping, piercing and punching. Typical uses include plum.. |
|||
Thermal Conductivity | 188.5 W/m-K | 1308 BTU-in/hr-ft²-°F | |
Eagle Brass 220 Commercial Bronze, Hard CDA 220 is known for having very good corrosion resistance, great cold workability and good hot workability for drawing, blanking, coining, stamping, piercing and punching. Typical uses include plum.. |
|||
Thermal Conductivity | 188.5 W/m-K | 1308 BTU-in/hr-ft²-°F | |
Eagle Brass 220 Commercial Bronze, Spring CDA 220 is known for having very good corrosion resistance, great cold workability and good hot workability for drawing, blanking, coining, stamping, piercing and punching. Typical uses include plum.. |
|||
Thermal Conductivity | 188.5 W/m-K | 1308 BTU-in/hr-ft²-°F | |
Chicago Extruded Metals BioBrass® UNS C22000 Copper-Zinc Alloy Finished product available as bar or wire.Chicago Extruded Metal temper codes: H01, H02, H04This alloy is registered with the U.S. EPA as Antimicrobial.Information provided by Chicago Extruded Metal.. |