Thermal Properties Metric English Comments
Thermal Conductivity 1.70 W/m-K
11.8 BTU-in/hr-ft²-°F
Along flow; ISO 22007-4
Victrex® PEEK 450FC30 General Purpose
Product Description: High performance thermoplastic material, 30% reinforced with carbon fibre / graphite / PTFE PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection molding and ext..
Thermal Conductivity 1.70 W/m-K
11.8 BTU-in/hr-ft²-°F
Laser flash method
LG Chemical LUCON CP510F PC/ABS+CNT
Description Injection Molding Grade, PC/ABS+CNT, Electrostatic Dissipation, High Flow, Good ProcessabilityApplication: Copy Machine Paper GuideCAS No. 103598-77-2 and 7440-44-0Information provided b..
Thermal Conductivity 1.70 W/m-K
11.8 BTU-in/hr-ft²-°F
Laser flash method
LG Chemical LUCON PN9008 PPS+MF+GF
Injection Molding Grade, PPS+MF+GF, High Thermal Conductivity, Chemical Resistance, High Heat ResistanceApplication: Electrical or Electronic Parts (Heat sink, LED etc.), Motor HousingsCAS No. 25212..
Thermal Conductivity 1.70 W/m-K
11.8 BTU-in/hr-ft²-°F
Longitudinal
LATI Laticonther 62 CPG/750 PA 6, Glass Fiber Reinforced
High thermal conductivity product based on Polyamide 6 (PA6). Special filler. Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided..
Thermal Conductivity 1.70 W/m-K
11.8 BTU-in/hr-ft²-°F
Longitudinal
LATI Latimass 62-07 D025 PA6, Impact Modified
Specific density compound based on Polyamide 6 (PA6), impact modified. Special filler.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by La..
Thermal Conductivity 1.70 W/m-K

@Temperature 90.0 °C
11.8 BTU-in/hr-ft²-°F

@Temperature 194 °F
DIN 51936, ASTM E 1461-01
Schott Nextrema® 712-3 Glass Ceramic
The NEXTREMA® family of glass-ceramics combines the glossy appearance of glass with exceptional thermal, chemical, optical and mechanical properties such as:Very low coefficient of linear thermal..
Thermal Conductivity 1.70 W/m-K

@Temperature 90.0 °C
11.8 BTU-in/hr-ft²-°F

@Temperature 194 °F
DIN 51936, ASTM E 1461-01
Schott Nextrema® 724-8 Glass Ceramic
The NEXTREMA® family of glass-ceramics combines the glossy appearance of glass with exceptional thermal, chemical, optical and mechanical properties such as:Very low coefficient of linear thermal..
Thermal Conductivity 1.70 W/m-K
11.8 BTU-in/hr-ft²-°F
Tra-Con Tra-Bond 293-14 Electrically Conductive Silver-Filled Epoxy Adhesive
TRA-BOND 293-14 silver-filled, electrically conductive epoxy adhesive is designed to provide strong bonds to difficult-to-bond metals, such as nickel, copper, gold and solder. The stress-absorbing c..
Thermal Conductivity 1.70 W/m-K
11.8 BTU-in/hr-ft²-°F
Dow Corning SE 4490 CV
One-part, white, non-flowing, highly filled compound, excellent thermal conductivity.Information provided by Dow Corning
Thermal Conductivity 1.70 W/m-K
11.8 BTU-in/hr-ft²-°F
China-Yixing Longly Refractories ASM-125 Cordierite-Mullite
Featured mullite, cordierite as the main raw material, the use of advanced production technology, professionally manufacturing the kiln furniture of ceramic and powder metallurgy with load bearing b..
Thermal Conductivity 1.70 W/m-K

@Pressure 30.0 MPa,
Temperature 50.0 °C
11.8 BTU-in/hr-ft²-°F

@Pressure 4350 psi,
Temperature 122 °F
Product Property; Arlon SQA-TMS-054
Arlon Thermabond® 48A43X008 0.008"(0.203 mm) Cured Silicone Rubber with Fiberglass Substrate
Description: Thermabond® Electrically insulating, thermally conductive, thermal interface material (TIM).Design/Construction: Side 1: Cured Silicone RubberSubstrate: Style 1080 FiberglassSide 2: Cu..
Thermal Conductivity 1.70 W/m-K

@Temperature 100 °C
11.8 BTU-in/hr-ft²-°F

@Temperature 212 °F
Silicone Property; ASTM E1530
Arlon Thermabond® R37300X008 0.008" Uncured Silicone Rubber on Fiberglass Carrier
Primerless Thermabond®: Electrically insulating, thermally conductive, electronic adhesive. Bonds without primer.Design/Construction:Liner: 1 mil FEPProduct: Uncured Silicone RubberCarrier: 3 m..
Thermal Conductivity 1.70 W/m-K
11.8 BTU-in/hr-ft²-°F
overall; Arlon SQA-TMS-054
Arlon R37879X034 Silicone Rubber/Fiberglass Laminate
Interleave: 3 mil PE; Layer 2: uncured silicone rubber; Layer 1: Cured silicone rubber; Substrate: 162 fiberglass
Thermal Conductivity 1.70 W/m-K
11.8 BTU-in/hr-ft²-°F
DIN EN 821-2 / ASTM-C408
CeramTec 447 Cordierite, 2MgO•Al2O3•5SiO2
Cordierites have low coefficients of thermal expansion and excellent resistance to thermal shock. They offer a range of thermal expansion, mechanical strength, and porosity criteria. They excel as c..
Thermal Conductivity 1.70 W/m-K
11.8 BTU-in/hr-ft²-°F
Along flow; ISO 22007-4
Victrex® PEEK 150FC30 Easy Flow
Product Description: High performance thermoplastic material, 30% reinforced with carbon fibre / graphite / PTFE PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection moulding, easy ..