Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 1.70 W/m-K | 11.8 BTU-in/hr-ft²-°F | Along flow; ISO 22007-4 |
Victrex® PEEK 450FC30 General Purpose Product Description: High performance thermoplastic material, 30% reinforced with carbon fibre / graphite / PTFE PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection molding and ext.. |
|||
Thermal Conductivity | 1.70 W/m-K | 11.8 BTU-in/hr-ft²-°F | Laser flash method |
LG Chemical LUCON CP510F PC/ABS+CNT Description Injection Molding Grade, PC/ABS+CNT, Electrostatic Dissipation, High Flow, Good ProcessabilityApplication: Copy Machine Paper GuideCAS No. 103598-77-2 and 7440-44-0Information provided b.. |
|||
Thermal Conductivity | 1.70 W/m-K | 11.8 BTU-in/hr-ft²-°F | Laser flash method |
LG Chemical LUCON PN9008 PPS+MF+GF Injection Molding Grade, PPS+MF+GF, High Thermal Conductivity, Chemical Resistance, High Heat ResistanceApplication: Electrical or Electronic Parts (Heat sink, LED etc.), Motor HousingsCAS No. 25212.. |
|||
Thermal Conductivity | 1.70 W/m-K | 11.8 BTU-in/hr-ft²-°F | Longitudinal |
LATI Laticonther 62 CPG/750 PA 6, Glass Fiber Reinforced High thermal conductivity product based on Polyamide 6 (PA6). Special filler. Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided.. |
|||
Thermal Conductivity | 1.70 W/m-K | 11.8 BTU-in/hr-ft²-°F | Longitudinal |
LATI Latimass 62-07 D025 PA6, Impact Modified Specific density compound based on Polyamide 6 (PA6), impact modified. Special filler.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by La.. |
|||
Thermal Conductivity | 1.70 W/m-K @Temperature 90.0 °C |
11.8 BTU-in/hr-ft²-°F @Temperature 194 °F |
DIN 51936, ASTM E 1461-01 |
Schott Nextrema® 712-3 Glass Ceramic The NEXTREMA® family of glass-ceramics combines the glossy appearance of glass with exceptional thermal, chemical, optical and mechanical properties such as:Very low coefficient of linear thermal.. |
|||
Thermal Conductivity | 1.70 W/m-K @Temperature 90.0 °C |
11.8 BTU-in/hr-ft²-°F @Temperature 194 °F |
DIN 51936, ASTM E 1461-01 |
Schott Nextrema® 724-8 Glass Ceramic The NEXTREMA® family of glass-ceramics combines the glossy appearance of glass with exceptional thermal, chemical, optical and mechanical properties such as:Very low coefficient of linear thermal.. |
|||
Thermal Conductivity | 1.70 W/m-K | 11.8 BTU-in/hr-ft²-°F | |
Tra-Con Tra-Bond 293-14 Electrically Conductive Silver-Filled Epoxy Adhesive TRA-BOND 293-14 silver-filled, electrically conductive epoxy adhesive is designed to provide strong bonds to difficult-to-bond metals, such as nickel, copper, gold and solder. The stress-absorbing c.. |
|||
Thermal Conductivity | 1.70 W/m-K | 11.8 BTU-in/hr-ft²-°F | |
Dow Corning SE 4490 CV One-part, white, non-flowing, highly filled compound, excellent thermal conductivity.Information provided by Dow Corning |
|||
Thermal Conductivity | 1.70 W/m-K | 11.8 BTU-in/hr-ft²-°F | |
China-Yixing Longly Refractories ASM-125 Cordierite-Mullite Featured mullite, cordierite as the main raw material, the use of advanced production technology, professionally manufacturing the kiln furniture of ceramic and powder metallurgy with load bearing b.. |
|||
Thermal Conductivity | 1.70 W/m-K @Pressure 30.0 MPa, Temperature 50.0 °C |
11.8 BTU-in/hr-ft²-°F @Pressure 4350 psi, Temperature 122 °F |
Product Property; Arlon SQA-TMS-054 |
Arlon Thermabond® 48A43X008 0.008"(0.203 mm) Cured Silicone Rubber with Fiberglass Substrate Description: Thermabond® Electrically insulating, thermally conductive, thermal interface material (TIM).Design/Construction: Side 1: Cured Silicone RubberSubstrate: Style 1080 FiberglassSide 2: Cu.. |
|||
Thermal Conductivity | 1.70 W/m-K @Temperature 100 °C |
11.8 BTU-in/hr-ft²-°F @Temperature 212 °F |
Silicone Property; ASTM E1530 |
Arlon Thermabond® R37300X008 0.008" Uncured Silicone Rubber on Fiberglass Carrier Primerless Thermabond®: Electrically insulating, thermally conductive, electronic adhesive. Bonds without primer.Design/Construction:Liner: 1 mil FEPProduct: Uncured Silicone RubberCarrier: 3 m.. |
|||
Thermal Conductivity | 1.70 W/m-K | 11.8 BTU-in/hr-ft²-°F | overall; Arlon SQA-TMS-054 |
Arlon R37879X034 Silicone Rubber/Fiberglass Laminate Interleave: 3 mil PE; Layer 2: uncured silicone rubber; Layer 1: Cured silicone rubber; Substrate: 162 fiberglass |
|||
Thermal Conductivity | 1.70 W/m-K | 11.8 BTU-in/hr-ft²-°F | DIN EN 821-2 / ASTM-C408 |
CeramTec 447 Cordierite, 2MgO•Al2O3•5SiO2 Cordierites have low coefficients of thermal expansion and excellent resistance to thermal shock. They offer a range of thermal expansion, mechanical strength, and porosity criteria. They excel as c.. |
|||
Thermal Conductivity | 1.70 W/m-K | 11.8 BTU-in/hr-ft²-°F | Along flow; ISO 22007-4 |
Victrex® PEEK 150FC30 Easy Flow Product Description: High performance thermoplastic material, 30% reinforced with carbon fibre / graphite / PTFE PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection moulding, easy .. |