Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 1.53 W/m-K | 10.6 BTU-in/hr-ft²-°F | |
Dow Corning SE 4486 SILICONE RTV One-part, white, moisture cure RTV, highly flowable, fast tack-free, high thermal conductivity, controlled volatility.Information provided by Dow Corning |
|||
Thermal Conductivity | 1.53 W/m-K | 10.6 BTU-in/hr-ft²-°F | |
Epoxy Technology EPO-TEK® E2036 Epoxy Product Description: A two component, slightly flexible, silver-filled, electrically conductive adhesive for semiconductor and electronic assemblies. It is a low Tg epoxy, intended for many kinds o.. |