Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 1.26 W/m-K | 8.74 BTU-in/hr-ft²-°F | |
Dow Corning SE 4445 CV KIT Two-part, grey, 1:1, addition cure gel, good thermal conductivity, controlled volatility, UL V-0.Information provided by Dow Corning |
|||
Thermal Conductivity | 1.26 W/m-K | 8.74 BTU-in/hr-ft²-°F | |
Dow Corning SE 4446 CV KIT Two-part, grey, 1:1, addition cure gel, good thermal conductivity, controlled volatility.Information provided by Dow Corning |