Thermal Properties Metric English Comments
Thermal Conductivity 0.930 W/m-K
6.45 BTU-in/hr-ft²-°F
DIN 52612
Fluorseals PTFE 15% graphite filled
Improved thermal conductivity and coefficient of friction.Information provided by TEKU GmbH Fluorkunststoffe, a distributor of Fluorseals materials.
Thermal Conductivity 0.930 W/m-K
6.45 BTU-in/hr-ft²-°F
Schott AF 45 Thin Borosilicate Glass
AF 45 is an alkali-free modified borosilicate glass with a high content of BaO and Al2O3. AF 45 with, its specific properties and large range of different thicknesses with tight tolerances, is exc..
Thermal Conductivity 0.930 W/m-K
6.45 BTU-in/hr-ft²-°F
Sharadaa Ceramics REFINSUL 11LI Insulating Castables Medium/High Purity
Description: We offer our clients Insulating Castables that are available in medium as well as high purity. Widely used in various industries, these are renowned for their strength and heat resistan..
Thermal Conductivity 0.930 W/m-K
6.45 BTU-in/hr-ft²-°F
Sharadaa Ceramics REFINSUL 15 Insulating Castables Medium/High Purity
Description: We offer our clients Insulating Castables that are available in medium as well as high purity. Widely used in various industries, these are renowned for their strength and heat resistan..
Thermal Conductivity 0.930 W/m-K
6.45 BTU-in/hr-ft²-°F
Sharadaa Ceramics REFINSUL 9 Insulating Castables Medium/High Purity
Description: We offer our clients Insulating Castables that are available in medium as well as high purity. Widely used in various industries, these are renowned for their strength and heat resistan..
Thermal Conductivity 0.930 W/m-K
6.45 BTU-in/hr-ft²-°F
Sharadaa Ceramics REFINSUL 13LI Insulating Castables Medium/High Purity
Description: We offer our clients Insulating Castables that are available in medium as well as high purity. Widely used in various industries, these are renowned for their strength and heat resistan..
Thermal Conductivity 0.930 W/m-K
6.45 BTU-in/hr-ft²-°F
Epoxy Technology EPO-TEK® E2001 Electrically Conductive, Silver-Filled Epoxy
Product Description: EPO-TEK® E2001 is a two component, silver-filled, electrically conductive epoxy designed for semiconductor die attach applications using a snap-cure profile. Advantages & Appl..
Thermal Conductivity 0.930 W/m-K
6.45 BTU-in/hr-ft²-°F
Epoxy Technology EPO-TEK® E3001 Electrically Conductive, Silver Epoxy