Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 0.131 W/m-K | 0.909 BTU-in/hr-ft²-°F | Melt |
Covestro Desmopan® W DP 85085A Polyurethane injection molding gradeno yellowing under the action of UV lightimproved microbial resistancegood low-temperature flexibilityImproved hydrolysis resistanceApplicationautomotive interior applications.. |