Polymer Property : Thermal Conductivity = 0.401 W/m-K Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Thermal Conductivity 0.401 W/m-K
2.78 BTU-in/hr-ft²-°F
ASTM D177
Premix Premi-Glas® 1265 VE 1265-VE (Compression Molded) Glass Reinforced Vinyl Ester TMC  (discontinued **)<
Description: Premi-Glas® 1265 VE is a glass reinforced vinyl ester molding compound designed for automotive under the hood applications. Key features and benefits: Designed for Injection or Injecti..
Thermal Conductivity 0.401 W/m-K
2.78 BTU-in/hr-ft²-°F
ASTM D177
Premix Premi-Glas® 1265 VE 1265-VE (Injection Compression Molded) Glass Reinforced Vinyl Ester TMC  (discontin
Description: Premi-Glas® 1265 VE is a glass reinforced vinyl ester molding compound designed for automotive under the hood applications. Key features and benefits: Designed for Injection or Injecti..
Thermal Conductivity 0.401 - 0.599 W/m-K
2.78 - 4.16 BTU-in/hr-ft²-°F
ASTM E1461-92
Park Electrochemical Nelco® N4000-11 BC® Buried Capacitance™ Epoxy Laminate and Prepreg
The Nelco® N4000-11 is a CAF resistant, high Tg (175º C by DSC) multifunctional epoxy dielectric substrate. This material is formulated to provide the PWB manufacturer and OEM with vastly improved..
Thermal Conductivity 0.401 - 0.599 W/m-K
2.78 - 4.16 BTU-in/hr-ft²-°F
ASTM E1461-92
Park Electrochemical Nelco® N4000-11 Multifunctional Epoxy Laminate and Prepreg
The Nelco® N4000-11 is a CAF resistant, high Tg (175º C by DSC) multifunctional epoxy dielectric substrate. This material is formulated to provide the PWB manufacturer and OEM with vastly improved..