Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 0.310 W/m-K | 2.15 BTU-in/hr-ft²-°F | |
Quadrant EPP Ertacetal® H POM-H, extruded (ISO Data) Ertacetal H is Quadrant’s homopolymer acetal grade. It offers a higher mechanical strength, stiffness, hardness and creep resistance as well as a lower thermal expansion rate and often also a bette.. |
|||
Thermal Conductivity | 0.310 W/m-K | 2.15 BTU-in/hr-ft²-°F | Average value: 0.310 W/m-K Grade Count:6 |
Overview of materials for Nylon 6, 30% Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 30% Mineral Filled". Specific grades with primary filler content between 25% and 34% are includ.. |
|||
Thermal Conductivity | 0.310 W/m-K | 2.15 BTU-in/hr-ft²-°F | ISO 8301:1991 |
Global EPP POM C Acetal Copolymer Polyacetals are highly crystalline thermoplastics, characterised by their high mechanical strength, rigidity and impact resistance. Acetal absorbs very little moisture, enabling the product to maint.. |
|||
Thermal Conductivity | 0.310 W/m-K | 2.15 BTU-in/hr-ft²-°F | |
Momentive Performance Materials RTV21 Pink General Purpose Potting/Encapsulating Compound Two-part condensation cure. Two-part condensation cure silicones RTVs are designed to cute at room temperature, and can be applied at temperature up to one inch (2.5 cm). These are very tough mate.. |
|||
Thermal Conductivity | 0.310 W/m-K | 2.15 BTU-in/hr-ft²-°F | |
Momentive Performance Materials RTV31 Red Extreme High Temperature Potting/Encapsulating Compound Two-part condensation cure. Two-part condensation cure silicones RTVs are designed to cute at room temperature, and can be applied at temperature up to one inch (2.5 cm). These are very tough mate.. |
|||
Thermal Conductivity | 0.310 W/m-K | 2.15 BTU-in/hr-ft²-°F | |
Momentive Performance Materials RTV31 Silicone Rubber Compound for High Temperature, Red RTV31, RTV60 and RTV88 silicone rubber compounds are high temperature two-part silicone elastomers. They are supplied ready-to-use with a base compound and DEBT (deputy tin deflagrate) as the standa.. |
|||
Thermal Conductivity | 0.310 W/m-K | 2.15 BTU-in/hr-ft²-°F | |
Momentive Performance Materials RTV627 Dark Gray General Purpose Potting/Encapsulating Compound Two-part addition cure. Two-part addition cure RTV silicones can be cured very quickly with the use of high heat. Addition cure products have no cure by-products and can be used to unlimited depth.. |
|||
Thermal Conductivity | 0.310 W/m-K | 2.15 BTU-in/hr-ft²-°F | |
Momentive Performance Materials RTV8262 Silicone Rubber Compounds for Potting, Encapsulating and Sealing RTV8111, RTV8112 and RTV8262 silicone rubber compounds are two-part silicone elastomers supplied in ready-to-use matched kits containing a base compound and curing agent.Mechanical and electrical pr.. |
|||
Thermal Conductivity | 0.310 W/m-K | 2.15 BTU-in/hr-ft²-°F | |
Momentive Performance Materials RTV560 Red Extreme High Temperature Potting/Encapsulating Compound Two-part condensation cure. Two-part condensation cure silicones RTVs are designed to cute at room temperature, and can be applied at temperature up to one inch (2.5 cm). These are very tough mate.. |
|||
Thermal Conductivity | 0.310 W/m-K | 2.15 BTU-in/hr-ft²-°F | |
Momentive Performance Materials RTV560 Silicone Rubber Compound for Low Temperature Potting, Encapsulating and Sealing, Red RTV511, RTV560 and RTV577 silicone rubber compounds are low temperature two-part silicone elastomers. They are supplied ready to use with a base compound and DBT (dibutyl tin dilaurate) as the stand.. |
|||
Thermal Conductivity | 0.310 W/m-K | 2.15 BTU-in/hr-ft²-°F | |
Momentive Performance Materials RTV60 Silicone Rubber Compound for High Temperature, Red RTV31, RTV60 and RTV88 silicone rubber compounds are high temperature two-part silicone elastomers. They are supplied ready-to-use with a base compound and DEBT (deputy tin deflagrate) as the standa.. |
|||
Thermal Conductivity | 0.310 W/m-K | 2.15 BTU-in/hr-ft²-°F | |
Momentive Performance Materials RTV6428 Dark Gray General Purpose Potting/Encapsulating Compound Two-part addition cure. Two-part addition cure RTV silicones can be cured very quickly with the use of high heat. Addition cure products have no cure by-products and can be used to unlimited depth.. |
|||
Thermal Conductivity | 0.310 W/m-K | 2.15 BTU-in/hr-ft²-°F | ASTM C177 |
SABIC Innovative Plastics ULTEM CRS5011R PEI (Europe-Africa-Middle East) Enhanced flow Polyetherimide copolymer (Tg 225C) with internal mold release and enhanced chemical resistance to strong acids, bases, aromatics and ketones. Resin is RoHS compliant. |
|||
Thermal Conductivity | 0.310 W/m-K | 2.15 BTU-in/hr-ft²-°F | ASTM C177 |
SABIC Innovative Plastics ULTEM UF5011S PEI Enhanced flow, Specialty filtered Polyetherimide (Tg 225C) with enhanced chemical resistance to strong acids, bases, aromatics and ketones. ECO Conforming. |
|||
Thermal Conductivity | 0.310 W/m-K | 2.15 BTU-in/hr-ft²-°F | ASTM C177 |
Solvay Specialty Polymers Ryton® R-4-220BL Polyphenylene Sulfide (PPS), 40% Glass Fiber Ryton® R-4-220NA and R-4-220BL 40% glass fiber reinforced polyphenylene sulfide compounds provide enhanced mechanical strength after constant or repeated exposure to high temperature water.Featur.. |
|||
Thermal Conductivity | 0.310 W/m-K | 2.15 BTU-in/hr-ft²-°F | ASTM C177 |
Solvay Specialty Polymers Ryton® R-4-222NA Polyphenylene Sulfide (PPS), 40% Glass Fiber Ryton® R-4-222NA 40% glass fiber reinforced polyphenylene sulfide compound provides enhanced mechanical strength after constant or repeated exposure to high temperature water and complies with Un.. |
|||
Thermal Conductivity | 0.310 W/m-K | 2.15 BTU-in/hr-ft²-°F | ASTM C177 |
Solvay Specialty Polymers Ryton® R-4-230BL Polyphenylene Sulfide (PPS), 40% Glass Fiber Ryton® R-4-230NA and R-4-230BL 40% glass fiber reinforced polyphenylene sulfide compounds provide reduced flash and improved processability compared to other polyphenylene sulfide injection moldi.. |
|||
Thermal Conductivity | 0.310 W/m-K | 2.15 BTU-in/hr-ft²-°F | ASTM C177 |
Solvay Specialty Polymers Ryton® R-4-240NA Polyphenylene Sulfide (PPS), 40% Glass Fiber Ryton® R-4-240NA and R-4-240BL 40% glass fiber reinforced polyphenylene sulfide compounds provide enhanced mechanical strength and toughness compared to other polyphenylene sulfide compounds.Feat.. |
|||
Thermal Conductivity | 0.310 W/m-K | 2.15 BTU-in/hr-ft²-°F | ASTM C177 |
Solvay Specialty Polymers Ryton® R-4-220NA Polyphenylene Sulfide (PPS), 40% Glass Fiber Ryton® R-4-220NA and R-4-220BL 40% glass fiber reinforced polyphenylene sulfide compounds provide enhanced mechanical strength after constant or repeated exposure to high temperature water.Featur.. |
|||
Thermal Conductivity | 0.310 W/m-K | 2.15 BTU-in/hr-ft²-°F | of melt |
DuPont Performance Polymers Zytel® FG70G50HSLA BK309 Nylon 66
(Unverified Data**) 50% Glass Reinforced Heat Stabilized Polyamide 66 with Developed for Food Contact Applications Information provided by DuPont Performance Polymers |
|||
Thermal Conductivity | 0.310 W/m-K | 2.15 BTU-in/hr-ft²-°F | Melt |
BASF Petra® 140 45% Glass Filled PET Petra 140 is a 45% glass reinforced injection molding polyethylene terephthalate (PET) offering an increased level of strength, stiffness, high temperature performance and dimensional stability. Ex.. |
|||
Thermal Conductivity | 0.310 W/m-K | 2.15 BTU-in/hr-ft²-°F | DIN 52612 |
BASF Ultramid® KR 4365 G5 BK 00100 35% Glass Filled PA6/6T FR (Conditioned) Description: Partially aromatic polyamide; flame retardant based on red phosphorus; low water absorption, high melting point (295°C); low tendency to form deposits on electrical contacts, very resi.. |
|||
Thermal Conductivity | 0.310 W/m-K | 2.15 BTU-in/hr-ft²-°F | DIN 52612 |
BASF Ultramid® KR 4365 G5 BK 00100 35% Glass Filled PA6/6T FR (Dry) Description: Partially aromatic polyamide; flame retardant based on red phosphorus; low water absorption, high melting point (295°C); low tendency to form deposits on electrical contacts, very resi.. |
|||
Thermal Conductivity | 0.310 W/m-K | 2.15 BTU-in/hr-ft²-°F | DIN 52612-1 |
BASF Ultramid® B3M6 BK 23213 30% Mineral Filled PA6 (Conditioned) Description: 30% Mineral-filled injection molding grade for high impact industrial items having very high dimensional stability, such as automobile wheel covers.Information provided by BASF |
|||
Thermal Conductivity | 0.310 W/m-K | 2.15 BTU-in/hr-ft²-°F | DIN 52612 |
CENTROPLAST CENTROGUARD Polyoxymethylene, Antimicrobial During the modification with POM CG, antimicrobial substances are included in the basic polyoxymethylene polymer, which provide an effective and long lasting solution against unwanted growth of micr.. |
|||
Thermal Conductivity | 0.310 W/m-K | 2.15 BTU-in/hr-ft²-°F | DIN 52612 |
BASF Ultramid® B3M6 BK60564 30% Mineral Filled PA6 (Dry) ultramid B3M6 BK60564 is a 30% mineral reinforced, pigmented black injection molding PA6 grade for industrial items requiring high impact strength and very high dimensional stability, excellent lase.. |
|||
Thermal Conductivity | 0.310 W/m-K | 2.15 BTU-in/hr-ft²-°F | |
CENTROPLAST CENTRODAL C Polyoxymethylene Copolymer CENTRODAL C is a versatile material with good chemical resistance, good machinability, and surface slip properties. Applications include sliding components and rollers, toothed wheels, ratchets, an.. |
|||
Thermal Conductivity | 0.310 W/m-K | 2.15 BTU-in/hr-ft²-°F | DIN 52612 |
CENTROPLAST CENTRODAL W Polyoxymethylene POM W is a semi-crystalline thermoplastic, which is certified in accordance with the regulatory system DVGW, technical regulations, work form W 270 and therefore, is particularly suited for the safe.. |
|||
Thermal Conductivity | 0.310 W/m-K | 2.15 BTU-in/hr-ft²-°F | |
Momentive Performance Materials RTV630 Blue General Purpose Potting/Encapsulating Compound Two-part addition cure. Two-part addition cure RTV silicones can be cured very quickly with the use of high heat. Addition cure products have no cure by-products and can be used to unlimited depth.. |
|||
Thermal Conductivity | 0.310 W/m-K | 2.15 BTU-in/hr-ft²-°F | DOM 52612 |
Manifattura Cattaneo POM c+PTFE Acetal, PTFE Filled Manifattura Cattaneo products are available in semi-finished forms such as bars, profiles, sheets and plates.Information provided by Manifattura Cattaneo s.p.a. |