Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 0.0390 W/m-K | 0.271 BTU-in/hr-ft²-°F | ISO 8301 |
3A Composites Core Materials AIREX® C70.130 Universal Structural Foam AIREX® C70 is a closed cell, crosslinked polymer foam that combines excellent stiffness and strength to weight ratios with superior toughness. It is non-friable, contains no CFC’s, has negli.. |
|||
Thermal Conductivity | 0.0390 W/m-K | 0.271 BTU-in/hr-ft²-°F | 15g/L; KS M 3808 |
LG Chemical R120 EPS, Flame Retardant Feature: Expendable Polystyrene, Flame RetardantApplication: Insulation Board, Sandwich Panel Civil Engineering & Construction MaterialsCAS No. 9003-53-6, 109-66-0, 3194-55-6 and 106-97-8Information.. |
|||
Thermal Conductivity | 0.0390 W/m-K | 0.271 BTU-in/hr-ft²-°F | mean temp of 10°C; ISO 8302 1991 |
Zotefoams Plastazote® LD30SD Static Dissipative Low Density Polyethylene Foam Plastazote® is a closed cell, cross-linked polyethylene foam manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and outs.. |
|||
Thermal Conductivity | 0.0390 W/m-K | 0.271 BTU-in/hr-ft²-°F | mean temp of 10°C; ISO 8302 1991 |
Zotefoams Plastazote® LD33FM Low Density Polyethylene Foam, Flame Retarded Plastazote® is a closed cell, cross-linked polyethylene foam manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and outs.. |
|||
Thermal Conductivity | 0.0390 W/m-K | 0.271 BTU-in/hr-ft²-°F | mean temp of 50°C; ISO 8301 |
Zotefoams ZOTEK® F 74 HT PVDF Foam Zotek® F 74 is a closed cell foam made from Arkema Kynar® PVDF manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and o.. |
|||
Thermal Conductivity | 0.0390 W/m-K | 0.271 BTU-in/hr-ft²-°F | mean temp of 10°C; ISO 8302 1991 |
Zotefoams Plastazote® LD29 Low Density Polyethylene Foam Plastazote® is a closed cell, cross-linked polyethylene foam manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and outs.. |
|||
Thermal Conductivity | 0.0390 W/m-K | 0.271 BTU-in/hr-ft²-°F | mean temp of 10°C; ISO 8302 1991 |
Zotefoams Plastazote® MP15FR Metallocene Polyethylene Foam, Flame Retardant Plastazote® is a closed cell, cross-linked polyethylene foam manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and outs.. |
|||
Thermal Conductivity | 0.0390 W/m-K | 0.271 BTU-in/hr-ft²-°F | mean temp of 10°C; ISO 8302 1991 |
Zotefoams Plastazote® MP24 Metallocene Polyethylene Foam Plastazote® is a closed cell, cross-linked polyethylene foam manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and outs.. |
|||
Thermal Conductivity | 0.0390 W/m-K | 0.271 BTU-in/hr-ft²-°F | mean temp of 10°C; ISO 8302 1991 |
Zotefoams Plastazote® MP33 Metallocene Polyethylene Foam Plastazote® is a closed cell, cross-linked polyethylene foam manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and outs.. |
|||
Thermal Conductivity | 0.0390 W/m-K | 0.271 BTU-in/hr-ft²-°F | DIN 52612 |
BASF Neopolen® P 8225 K 0.05 g/cc Core density; Expanded Polypropylene (Europe) Description: Neopolen® P 8225 K is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 8225 K.Note: In order to.. |
|||
Thermal Conductivity | 0.0390 W/m-K | 0.271 BTU-in/hr-ft²-°F | DIN 52612 |
BASF Neopolen® P 9035 0.05 g/cc Core density; Expanded Polypropylene (Europe) Description: Neopolen® P 9035 is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 9035.Note: In order to mea.. |
|||
Thermal Conductivity | 0.0390 W/m-K | 0.271 BTU-in/hr-ft²-°F | DIN 52612 |
BASF Neopolen® P 9225 K 0.05 g/cc Core density; Expanded Polypropylene (Europe) Description: Neopolen® P 9225 K is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 9225 K.Note: In order to.. |
|||
Thermal Conductivity | 0.0390 W/m-K | 0.271 BTU-in/hr-ft²-°F | DIN 52612 |
BASF Neopolen® P 9230 K 0.05 g/cc Core density; Expanded Polypropylene (Europe) Description: Neopolen® P 9230 K is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 9230 K.Note: In order to.. |
|||
Thermal Conductivity | 0.0390 W/m-K | 0.271 BTU-in/hr-ft²-°F | DIN 52612 |
BASF Neopolen® P 9335 MG 0.07 g/cc Core density; Expanded Polypropylene (Europe) Description: Neopolen® P 9333 MG is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 9333 MG.Note: In order .. |
|||
Thermal Conductivity | 0.0390 W/m-K | 0.271 BTU-in/hr-ft²-°F | DIN 52612 |
BASF Neopolen® P 9435 0.05 g/cc Core density; Expanded Polypropylene (Europe) Description: Neopolen® P 9435 is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 9435.Note: In order to mea.. |
|||
Thermal Conductivity | 0.0390 W/m-K | 0.271 BTU-in/hr-ft²-°F | Moisture Content: 10% |
BASF Styrodur® 3035 CS Extruded Rigid Polystyrene Foam (Europe) Description: Styrodur C is the green extruded rigid polystyrene foam (XPS) from BASF. As a thermal insulation, it makes a significant contribution to climate protection by reducing CO2 emissions. Th.. |
|||
Thermal Conductivity | 0.0390 W/m-K | 0.271 BTU-in/hr-ft²-°F | Moisture Content: 10% |
BASF Styrodur® 4000 CS Extruded Rigid Polystyrene Foam (Europe) Description: Styrodur C is the green extruded rigid polystyrene foam (XPS) from BASF. As a thermal insulation, it makes a significant contribution to climate protection by reducing CO2 emissions. Th.. |
|||
Thermal Conductivity | 0.0390 W/m-K | 0.271 BTU-in/hr-ft²-°F | Moisture Content: 10% |
BASF Styrodur® 5000 CS Extruded Rigid Polystyrene Foam (Europe) Description: Styrodur C is the green extruded rigid polystyrene foam (XPS) from BASF. As a thermal insulation, it makes a significant contribution to climate protection by reducing CO2 emissions. Th.. |
|||
Thermal Conductivity | 0.0390 W/m-K | 0.271 BTU-in/hr-ft²-°F | ISO 8301 |
3A Composites Core Materials AIREX® R63.140 Damage Tolerant Foam AIREX® R63 is a closed-cell, linear, thermoplastic polymer foam with extremely high damage tolerance. This formula combines high elongation and excellent bond strength. AIREX® R63 is cold formable.. |
|||
Thermal Conductivity | 0.0390 W/m-K | 0.271 BTU-in/hr-ft²-°F | DIN 52612 |
BASF Neopolen® P 9235 0.05 g/cc Core density; Expanded Polypropylene (Europe) Description: Neopolen® P 9235 is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 9235.Note: In order to mea.. |
|||
Thermal Conductivity | 0.0390 W/m-K | 0.271 BTU-in/hr-ft²-°F | DIN 52612 |
BASF Neopolen® P 9435 0.07 g/cc Core density; Expanded Polypropylene (Europe) Description: Neopolen® P 9435 is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 9435.Note: In order to mea.. |
|||
Thermal Conductivity | 0.0390 W/m-K | 0.271 BTU-in/hr-ft²-°F | Moisture Content: 10% |
BASF Styrodur® 2500 C Extruded Rigid Polystyrene Foam (Europe) Description: Styrodur C is the green extruded rigid polystyrene foam (XPS) from BASF. As a thermal insulation, it makes a significant contribution to climate protection by reducing CO2 emissions. Th.. |
|||
Thermal Conductivity | 0.0390 W/m-K | 0.271 BTU-in/hr-ft²-°F | Moisture Content: 10% |
BASF Styrodur® 2800 C Extruded Rigid Polystyrene Foam (Europe) Description: Styrodur C is the green extruded rigid polystyrene foam (XPS) from BASF. As a thermal insulation, it makes a significant contribution to climate protection by reducing CO2 emissions. Th.. |
|||
Thermal Conductivity | 0.0390 W/m-K | 0.271 BTU-in/hr-ft²-°F | Moisture Content: 10% |
BASF Styrodur® 3035 CN Extruded Rigid Polystyrene Foam (Europe) Description: Styrodur C is the green extruded rigid polystyrene foam (XPS) from BASF. As a thermal insulation, it makes a significant contribution to climate protection by reducing CO2 emissions. Th.. |