Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 0.259 W/m-K | 1.80 BTU-in/hr-ft²-°F | ASTM F433 |
Quadrant EPP Duratron® PAI T4203 Extruded Polyamide-imide (ASTM Product Data Sheet) |
|||
Thermal Conductivity | 0.259 - 0.331 W/m-K | 1.80 - 2.30 BTU-in/hr-ft²-°F | |
Polygon Polylube™ Fiber Series Epoxy Composite Bearings Low friction coupled with high load carrying capacity are natural benefits. Teflon® superfilaments, which exhibit tensile strength twenty times greater than PTFE resins are integrated into the bea.. |
|||
Thermal Conductivity | 0.259 W/m-K | 1.80 BTU-in/hr-ft²-°F | ASTM F433 |
Quadrant EPP Duratron® PAI T4503 Compression Molded, Polyamide-imide, Eelectrical Grade (ASTM Product Data Sheet) |
|||
Thermal Conductivity | 0.259 W/m-K | 1.80 BTU-in/hr-ft²-°F | ASTM F433 |
Quadrant EPP Quadrant LSG PSU, Extruded, Unfilled, Polysulfone (ASTM Product Data Sheet) |
|||
Thermal Conductivity | 0.259 W/m-K | 1.80 BTU-in/hr-ft²-°F | |
Quadrant EPP Semitron® CMP XL20 (ASTM Product Data Sheet) |
|||
Thermal Conductivity | 0.259 W/m-K | 1.80 BTU-in/hr-ft²-°F | ASTM C177 |
Quantum PET Information provided by Quantum Advanced Engineering Plastics |
|||
Thermal Conductivity | 0.259 W/m-K | 1.80 BTU-in/hr-ft²-°F | Average value: 0.259 W/m-K Grade Count:3 |
Overview of materials for Polyetherimide (PEI), 40% Glass Fiber This property data is a summary of similar materials in the MatWeb database for the category "Polyetherimide, 40% Glass Fiber". Specific grades with glass content between 35% and 44% are included. E.. |
|||
Thermal Conductivity | 0.259 - 0.540 W/m-K | 1.80 - 3.75 BTU-in/hr-ft²-°F | Average value: 0.392 W/m-K Grade Count:6 |
Overview of materials for Polyamide-Imide, Molded This property data is a summary of similar materials in the MatWeb database for the category "Polyamide-Imide, Molded". Each property range of values reported is minimum and maximum values of approp.. |
|||
Thermal Conductivity | 0.259 - 1.26 W/m-K | 1.80 - 8.72 BTU-in/hr-ft²-°F | Average value: 0.795 W/m-K Grade Count:7 |
Overview of materials for Epoxy, Encapsulating, Glass or Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Epoxy, Encapsulating, Glass or Mineral Filled". Each property range of values reported is minimum and ma.. |
|||
Thermal Conductivity | 0.259 - 0.576 W/m-K | 1.80 - 4.00 BTU-in/hr-ft²-°F | Average value: 0.398 W/m-K Grade Count:26 |
Overview of materials for Nylon 612, Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Nylon 612, Glass Fiber Filler". Each property range of values reported is minimum and maximum values of .. |
|||
Thermal Conductivity | 0.259 W/m-K | 1.80 BTU-in/hr-ft²-°F | |
Saint-Gobain Rulon® 1410 Grade Bearing/Seal PTFE Description: Rulon® is the Saint-Gobain trade name for their family of proprietary PTFE compounds. This family of materials offers the combination of high compressive strength, low coefficient of.. |
|||
Thermal Conductivity | 0.259 W/m-K | 1.80 BTU-in/hr-ft²-°F | ASTM C177 |
Westlake Plastics Tempalux® 30% GF Polyetherimide An amorphous thermoplastic polyetherimide, stock shapes from ULTEM® resin possess a combination of useful characteristics, including high strength at elevated temperatures, high modulus, and broad .. |
|||
Thermal Conductivity | 0.259 W/m-K | 1.80 BTU-in/hr-ft²-°F | ASTM F433 |
Quadrant EPP Quadrant PSU Estruded Unfilled Polysulfone (ASTM Product Data Sheet) |
|||
Thermal Conductivity | 0.259 W/m-K | 1.80 BTU-in/hr-ft²-°F | ASTM C177 |
Quantum PEI - Ultem® 30% Glass Fiber Filled Information provided by Quantum Advanced Engineering Plastics |