Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 0.0310 W/m-K @Thickness 30.0 mm |
0.215 BTU-in/hr-ft²-°F @Thickness 1.18 in |
DIN EN 13164 |
BASF Styrodur® 3035 CS Extruded Rigid Polystyrene Foam (Europe) Description: Styrodur C is the green extruded rigid polystyrene foam (XPS) from BASF. As a thermal insulation, it makes a significant contribution to climate protection by reducing CO2 emissions. Th.. |
|||
Thermal Conductivity | 0.0310 W/m-K @Thickness 30.0 mm |
0.215 BTU-in/hr-ft²-°F @Thickness 1.18 in |
DIN EN 13164 |
BASF Styrodur® 4000 CS Extruded Rigid Polystyrene Foam (Europe) Description: Styrodur C is the green extruded rigid polystyrene foam (XPS) from BASF. As a thermal insulation, it makes a significant contribution to climate protection by reducing CO2 emissions. Th.. |
|||
Thermal Conductivity | 0.0310 W/m-K @Thickness 30.0 mm |
0.215 BTU-in/hr-ft²-°F @Thickness 1.18 in |
DIN EN 13164 |
BASF Styrodur® 2500 C Extruded Rigid Polystyrene Foam (Europe) Description: Styrodur C is the green extruded rigid polystyrene foam (XPS) from BASF. As a thermal insulation, it makes a significant contribution to climate protection by reducing CO2 emissions. Th.. |
|||
Thermal Conductivity | 0.0310 W/m-K @Thickness 30.0 mm |
0.215 BTU-in/hr-ft²-°F @Thickness 1.18 in |
DIN EN 13164 |
BASF Styrodur® 2800 C Extruded Rigid Polystyrene Foam (Europe) Description: Styrodur C is the green extruded rigid polystyrene foam (XPS) from BASF. As a thermal insulation, it makes a significant contribution to climate protection by reducing CO2 emissions. Th.. |
|||
Thermal Conductivity | 0.0310 W/m-K @Thickness 30.0 mm |
0.215 BTU-in/hr-ft²-°F @Thickness 1.18 in |
DIN EN 13164 |
BASF Styrodur® 3035 CN Extruded Rigid Polystyrene Foam (Europe) Description: Styrodur C is the green extruded rigid polystyrene foam (XPS) from BASF. As a thermal insulation, it makes a significant contribution to climate protection by reducing CO2 emissions. Th.. |
|||
Thermal Conductivity | 0.0310 W/m-K | 0.215 BTU-in/hr-ft²-°F | ISO 8301 |
3A Composites Core Materials AIREX® C70.40 Universal Structural Foam AIREX® C70 is a closed cell, crosslinked polymer foam that combines excellent stiffness and strength to weight ratios with superior toughness. It is non-friable, contains no CFC’s, has negligible .. |
|||
Thermal Conductivity | 0.0310 W/m-K | 0.215 BTU-in/hr-ft²-°F | ISO 8301 |
3A Composites Core Materials AIREX® C70.48 Universal Structural Foam AIREX® C70 is a closed cell, crosslinked polymer foam that combines excellent stiffness and strength to weight ratios with superior toughness. It is non-friable, contains no CFC’s, has negligible .. |
|||
Thermal Conductivity | 0.0310 W/m-K | 0.215 BTU-in/hr-ft²-°F | ISO 8301 |
3A Composites Core Materials AIREX® C70.55 Universal Structural Foam AIREX® C70 is a closed cell, crosslinked polymer foam that combines excellent stiffness and strength to weight ratios with superior toughness. It is non-friable, contains no CFC’s, has negligible .. |
|||
Thermal Conductivity | 0.0310 W/m-K | 0.215 BTU-in/hr-ft²-°F | ISO 8301 |
3A Composites Core Materials AIREX® C71.55 Elevated Temperature Structural Foam AIREX® C71 is a closed cell, crosslinked polymer foam especially formulated to maintain its stability also at higher processing or service temperatures. It combines excellent stiffness and strength.. |