Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 0.209 W/m-K | 1.45 BTU-in/hr-ft²-°F | |
Honeywell ACLAR® 11A (8.00 mil) CTFE Homopolymer, Barrier Film
(discontinued **) Description: ACLAR® 11A is a CTFE homopolymer, high performance barrier film for industrial and electronics applications.Information provided by Honeywell. |
|||
Thermal Conductivity | 0.209 W/m-K | 1.45 BTU-in/hr-ft²-°F | |
Honeywell ACLAR® 11A (4.00 mil) CTFE Homopolymer, Barrier Film
(discontinued **) Description: ACLAR® 11A is a CTFE homopolymer, high performance barrier film for industrial and electronics applications.Information provided by Honeywell. |
|||
Thermal Conductivity | 0.209 W/m-K | 1.45 BTU-in/hr-ft²-°F | |
Honeywell ACLAR® 11A (3.00 mil) CTFE Homopolymer, Barrier Film
(discontinued **) Description: ACLAR® 11A is a CTFE homopolymer, high performance barrier film for industrial and electronics applications.Information provided by Honeywell. |
|||
Thermal Conductivity | 0.209 W/m-K | 1.45 BTU-in/hr-ft²-°F | |
Honeywell ACLAR® 11A (2.00 mil) CTFE Homopolymer, Barrier Film
(discontinued **) Description: ACLAR® 11A is a CTFE homopolymer, high performance barrier film for industrial and electronics applications.Information provided by Honeywell. |
|||
Thermal Conductivity | 0.209 W/m-K | 1.45 BTU-in/hr-ft²-°F | |
Honeywell ACLAR® 11A (0.90 mil) CTFE Homopolymer, Barrier Film
(discontinued **) Description: ACLAR® 11A is a CTFE homopolymer, high performance barrier film for industrial and electronics applications.Information provided by Honeywell. |
|||
Thermal Conductivity | 0.209 W/m-K | 1.45 BTU-in/hr-ft²-°F | |
Honeywell ACLAR® 11A(0.60 mil) CTFE Homopolymer, Barrier Film
(discontinued **) Description: ACLAR® 11A is a CTFE homopolymer, high performance barrier film for industrial and electronics applications.Information provided by Honeywell. |
|||
Thermal Conductivity | 0.209 W/m-K | 1.45 BTU-in/hr-ft²-°F | |
Momentive Performance Materials RTV102 One Component Acetoxy Adhesive Sealant, White RTV series one-component, ready-to-use adhesive sealants are extremely versatile. They cure to a tough, durable, resilient silicone rubber on exposure to atmospheric moisture at room temperature. .. |
|||
Thermal Conductivity | 0.209 W/m-K | 1.45 BTU-in/hr-ft²-°F | |
Momentive Performance Materials RTV103 One Component Acetoxy Adhesive Sealant, Black RTV series one-component, ready-to-use adhesive sealants are extremely versatile. They cure to a tough, durable, resilient silicone rubber on exposure to atmospheric moisture at room temperature. .. |
|||
Thermal Conductivity | 0.209 W/m-K | 1.45 BTU-in/hr-ft²-°F | |
Momentive Performance Materials RTV106 One Component Acetoxy Adhesive Sealant, Red RTV series one-component, ready-to-use adhesive sealants are extremely versatile. They cure to a tough, durable, resilient silicone rubber on exposure to atmospheric moisture at room temperature. .. |
|||
Thermal Conductivity | 0.209 W/m-K | 1.45 BTU-in/hr-ft²-°F | |
Momentive Performance Materials RTV108 One Component Acetoxy Adhesive Sealant, Translucent RTV series one-component, ready-to-use adhesive sealants are extremely versatile. They cure to a tough, durable, resilient silicone rubber on exposure to atmospheric moisture at room temperature. .. |
|||
Thermal Conductivity | 0.209 W/m-K | 1.45 BTU-in/hr-ft²-°F | |
Momentive Performance Materials RTV109 One Component Acetoxy Adhesive Sealant, Aluminum RTV series one-component, ready-to-use adhesive sealants are extremely versatile. They cure to a tough, durable, resilient silicone rubber on exposure to atmospheric moisture at room temperature. .. |
|||
Thermal Conductivity | 0.209 W/m-K | 1.45 BTU-in/hr-ft²-°F | |
Momentive Performance Materials RTV112 One Component Acetoxy Adhesive Sealant, White RTV series one-component, ready-to-use adhesive sealants are extremely versatile. They cure to a tough, durable, resilient silicone rubber on exposure to atmospheric moisture at room temperature. .. |
|||
Thermal Conductivity | 0.209 W/m-K | 1.45 BTU-in/hr-ft²-°F | |
Momentive Performance Materials RTV116 One Component Acetoxy Adhesive Sealant, Red RTV series one-component, ready-to-use adhesive sealants are extremely versatile. They cure to a tough, durable, resilient silicone rubber on exposure to atmospheric moisture at room temperature. .. |
|||
Thermal Conductivity | 0.209 W/m-K | 1.45 BTU-in/hr-ft²-°F | |
Momentive Performance Materials RTV118 One Component Acetoxy Adhesive Sealant, Translucent RTV series one-component, ready-to-use adhesive sealants are extremely versatile. They cure to a tough, durable, resilient silicone rubber on exposure to atmospheric moisture at room temperature. .. |
|||
Thermal Conductivity | 0.209 W/m-K | 1.45 BTU-in/hr-ft²-°F | |
Momentive Performance Materials RTV157 High Strength Silicone Adhesive Sealant, Gray RTV 157 is a one component, ready-to-use, high strength silicone rubber adhesive sealant. It cures to tough resilient silicone rubber on exposure to atmospheric moisture at room temperature. RTV15.. |
|||
Thermal Conductivity | 0.209 W/m-K | 1.45 BTU-in/hr-ft²-°F | |
Momentive Performance Materials RTV159 High Strength Silicone Adhesive Sealant, Red RTV 159 is a one component, ready-to-use, high strength silicone rubber adhesive sealant. It cures to tough resilient silicone rubber on exposure to atmospheric moisture at room temperature. RTV15.. |
|||
Thermal Conductivity | 0.209 W/m-K | 1.45 BTU-in/hr-ft²-°F | |
Momentive Performance Materials RTV160 Electronic Grade Silicone Adhesive Sealant, White RTV160, RTV162, and RTV 167 adhesive sealants for GE silicones are one-component, ready-to-use electronic grade silicone sealants. They cure to a tough, resilient silicone rubber on exposure to atm.. |
|||
Thermal Conductivity | 0.209 W/m-K | 1.45 BTU-in/hr-ft²-°F | |
Momentive Performance Materials RTV162 Electronic Grade Silicone Adhesive Sealant, White RTV160, RTV162, and RTV 167 adhesive sealants for GE silicones are one-component, ready-to-use electronic grade silicone sealants. They cure to a tough, resilient silicone rubber on exposure to atm.. |
|||
Thermal Conductivity | 0.209 W/m-K | 1.45 BTU-in/hr-ft²-°F | |
Momentive Performance Materials RTV167 Electronic Grade Silicone Adhesive Sealant, Gray RTV160, RTV162, and RTV 167 adhesive sealants for GE silicones are one-component, ready-to-use electronic grade silicone sealants. They cure to a tough, resilient silicone rubber on exposure to atm.. |
|||
Thermal Conductivity | 0.209 W/m-K | 1.45 BTU-in/hr-ft²-°F | |
Momentive Performance Materials RTV1673LV One Component, Low Volatile Silicone Adhesive Sealant, Black RTV1673LV one-component, ready-to-use adhesive sealants cures to a tough durable, resilient silicone rubber when exposed to atmospheric moisture at room temperature. Methyl alcohol and a small amoun.. |
|||
Thermal Conductivity | 0.209 W/m-K | 1.45 BTU-in/hr-ft²-°F | ASTM C177-76 |
Lucite International XL Sanitary Ware Acrylic Sheet Lucite® XL continuous-cast cross-linked acrylic sheet is specially formulated for deep-draw thermoforming. It is used primarily for production of spas.Benefits: Smooth surface; Infinite colors an.. |
|||
Thermal Conductivity | 0.209 W/m-K | 1.45 BTU-in/hr-ft²-°F | Cento-Fitch |
Spartech Polycast SAR (Super Abrasion Resistant) Cell Cast Acrylic Description: Cell Cast AcrylicInformation provided by Spartech. |
|||
Thermal Conductivity | 0.209 W/m-K | 1.45 BTU-in/hr-ft²-°F | ASTM D177 |
Diapolyacrylate Acrypet® MF-001 PMMA Acrypet® is a registered trade mark of Diapolyacrylate Company Limited. Information provided by Dayson Polymers. |
|||
Thermal Conductivity | 0.209 W/m-K | 1.45 BTU-in/hr-ft²-°F | ASTM D177 |
Diapolyacrylate Acrypet® VH-001 Heat Stabilized PMMA Acrypet® is a registered trade mark of Diapolyacrylate Company Limited. Information provided by Dayson Polymers. |
|||
Thermal Conductivity | 0.209 W/m-K | 1.45 BTU-in/hr-ft²-°F | ASTM D177 |
Diapolyacrylate Acrypet® IR H70 Impact Modified PMMA Acrypet® is a registered trade mark of Diapolyacrylate Company Limited. Information provided by Dayson Polymers. |
|||
Thermal Conductivity | 0.209 W/m-K | 1.45 BTU-in/hr-ft²-°F | |
3M Scotch-Weld™ 2214 Non-Metallic Filled Epoxy Adhesive 3M™ Scotch-Weld™ Non-Metallic Filled is a non-metal filled version of Scotch-Weld adhesive 2214 regular. One part 250°F (121°C) curing 100% solids, 3M™ Scotch-Weld™ Epoxy Adhesive 2214 is a pa.. |
|||
Thermal Conductivity | 0.209 W/m-K | 1.45 BTU-in/hr-ft²-°F | |
Arlon R33889R020 0.020" (0.508 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Layer-on-Layer This data Represents typical values for the production material. The data should not be used to write, or in place of, material specifications.Information .. |