Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Thermal Conductivity = 0.191 W/m-K Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Thermal Conductivity 0.191 - 0.663 W/m-K
1.33 - 4.60 BTU-in/hr-ft²-°F
Average value: 0.239 W/m-K Grade Count:16
Overview of materials for Polycarbonate, 10% Glass Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, 10% Glass Filled". Specific grades with glass content between 5% and 14% are included. Ea..
Thermal Conductivity 0.191 W/m-K
1.33 BTU-in/hr-ft²-°F
Styron CALIBREâ„¢ IM 401 11 Polycarbonate, Impact Modified
CALIBRE® IM401 series resins are impact modified, UL listed polycarbonate resins which contain mold release. CALIBRE IM401 polycarbonate resins exhibit an excellent balance of impact strength and..
Thermal Conductivity 0.191 W/m-K
1.33 BTU-in/hr-ft²-°F
Melt
Covestro Makrolon® 8315 Polycarbonate, 10% Glass Filled
MVR (300 °C/1.2 kg) 6.0 cm3/10 minhigh viscosityeasy releaseinjection moldingavailable in opaque colors onlyPreprocessingMax. Water content
Thermal Conductivity 0.191 W/m-K
1.33 BTU-in/hr-ft²-°F
Melt
Covestro Makrolon® 9415 Polycarbonate, 10% Glass Filled
ISO 7391-PC,MFR,(,,)-09-9,GF10Global gradeMVR (300 °C/1.2 kg) 6.0 cm3/10 min10 % Glass fiber reinforcedChlorine- and bromine-free flame retardantUL 94V-0/1.5 mm and 5VA/3.0 mmHigh viscosityEasy rel..
Thermal Conductivity 0.191 W/m-K
1.33 BTU-in/hr-ft²-°F
Melt
Covestro Makrolon® 9417 Polycarbonate, 10% Glass Filled
ISO 7391-PC,MFLR,(,,)-09-9,GF10Global gradeMVR (300 °C/1.2 kg) 6.0 cm3/10 min10 % Glass fiber reinforcedChlorine- and bromine-free flame retardantUL 94V-0/1.5 mm and 5VA/3.0 mmHigh viscosityUV stab..
Thermal Conductivity 0.191 W/m-K
1.33 BTU-in/hr-ft²-°F
Melt
Covestro Makrolon® GF9002* Polycarbonate, 10% Glass Filled
ISO 7391-PC,MFR,(,,)-18-9,GF10Formerly Makrolon DP1-1889MVR (300 °C/1.2 kg) 15 cm3/10 min10 % Glass fiber reinforcedChlorine- and bromine-free flame retardantUL 94V-0/1.2 mmUL 94 5VA/2.8 mm (Bayer ..
Thermal Conductivity 0.191 W/m-K
1.33 BTU-in/hr-ft²-°F
Melt
Covestro Makrolon® DP1-1887* Polycarbonate, 10% Glass Filled
ISO 7391-PC,MR,(,,)-18-9,GF10Developmental productMVR (300 °C/1.2 kg) 16 cm3/10 min10 % Glass fiber reinforcedMilled fiberLow viscosityEasy releasegood surface qualityInjection molding - Melt tempe..
Copyright © lookpolymers.com All Rights Reserved