Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 0.174333 W/m-K | 1.20987 BTU-in/hr-ft²-°F | ASTM C177 |
Mitsui AURUM® PL450C Polyimide
(discontinued **) AURUM PL450C is a high performance thermoplastic polyimide for precision injection molded components and extruded products. A member of the AURUM family of advanced engineering resins, unfilled AURU.. |