Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Thermal Conductivity = 0.130 W/m-K Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Thermal Conductivity 0.130 W/m-K
0.902 BTU-in/hr-ft²-°F
ASTM C177
Plaskolite Optix® Acrylic Sheet
Optix® is a continuously processed acrylic sheet that is crystal clear, impact resistant, weather resistant, and non-yellowing. It offers high molecular weight for superior thermoforming, bending,..
Thermal Conductivity 0.130 W/m-K
0.902 BTU-in/hr-ft²-°F
ASTM C177
SABIC Innovative Plastics Lexan® FL910 PC
Various weight reductions at 0.250"" (6.35 mm) wall, 10% GR. High flexural strength and modulus, impact/heat resistant. V-0/5V at 0.250"" (6.35 mm).
Thermal Conductivity 0.130 W/m-K
0.902 BTU-in/hr-ft²-°F
ASTM C177
SABIC Innovative Plastics Lexan® FL913 PC
Various weight reduction at 0.250"" (6.35 mm) wall. 10% GR, high flexural strength/modulus. UL rated V-0/5VA (all except natural). UV-stabilized.
Thermal Conductivity 0.130 W/m-K
0.900 BTU-in/hr-ft²-°F
ASTM C177
Plaskolite Optix® DA Digital Acrylic Sheet
Designed to provide optimal adhesion of UV curing inks without adhesion promoters, OPTIX DA is a continuously processed acrylic sheet specially formulated product for printing. OPTIX DA provides sup..
Thermal Conductivity 0.130 W/m-K
0.902 BTU-in/hr-ft²-°F
DIN 52612
GEHR Plastics PVDF Polyvinylidene Fluoride
Polyvinylidene fluoride shows a higher tensile strength, pressure resistance and dimensional stability than the related PTFE, but friction and insulation properties are lower. PVDF has a high mechan..
Thermal Conductivity 0.130 W/m-K
0.902 BTU-in/hr-ft²-°F
Melt; ASTM C177
Styron MAGNUMâ„¢ 357 HP Acrylonitrile Butadiene Styrene (ABS) Resin
Overview: MAGNUMâ„¢ ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositi..
Thermal Conductivity 0.130 W/m-K

@Temperature 650 °C
0.902 BTU-in/hr-ft²-°F

@Temperature 1200 °F
ASTM-C177
Unifrax CC-Max® 4 HP Substrate Support Mat
CC-Max 4 HP mat is produced when the proprietary fiber is converted into a flexible flet-like product. The material is thermally stable and engineered to maintain a controlled holding force on the ..
Thermal Conductivity 0.130 W/m-K
0.902 BTU-in/hr-ft²-°F
Tra-Con Tra-Cast 3110 Low Density Epoxy Casting System
TRA-CAST 3110 is a unicellular, low density, syntactic-foam epoxy resin casting system of medium viscosity that easily handles, mixes and cures at room temperature. Developed for industrial encapsul..
Thermal Conductivity 0.130 W/m-K
0.902 BTU-in/hr-ft²-°F
Trelleborg Offshore Vikotherm™ 73585 Insulative Elastomer
Vikotherm™ is a rubber elastomer chemically modified to provide very high insulating characteristics while maintaining its inherent rubber properties in respect of seawater resistance, pressure res..
Thermal Conductivity 0.130 W/m-K
0.902 BTU-in/hr-ft²-°F
Tra-Con Tra-Bond 2125 Rigid Syntactic Repair Adhesive
TRA-BOND 2125 is a medium viscosity, low density syntactic foam epoxy formulation developed for industrial, electronic and aerospace honeycomb, fillet, edge-fill, contour repair, bonding and casting..
Thermal Conductivity 0.130 W/m-K
0.902 BTU-in/hr-ft²-°F
CMT Materials HYTAC® C1R Highly Durable Syntactic Foam, Dust-Free Machining/Polishing
HYTAC-C1R is easily machined without the dust typically associated with epoxy syntactic foam. This new copolymer base has been optimized for both the machine shop and the thermoforming process.Exce..
Thermal Conductivity 0.130 - 0.170 W/m-K
0.902 - 1.18 BTU-in/hr-ft²-°F
Abatron AboCast/AboCure 8109-11
All-purpose, structural dielectric resin. Better thermal and chemical properties than 8109-8, but requires heat cure. Melts at 70-80°C and remains liquid (supercooled) for many hours at RT.Process..
Thermal Conductivity 0.130 - 0.190 W/m-K
0.900 - 1.32 BTU-in/hr-ft²-°F
Average value: 0.160 W/m-K Grade Count:4
Overview of materials for Acrylic, Optical Sheet
This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, Optical Sheet". Each property range of values reported is minimum and maximum values of appropr..
Copyright © lookpolymers.com All Rights Reserved