Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 0.0370 - 0.700 W/m-K | 0.257 - 4.86 BTU-in/hr-ft²-°F | Average value: 0.378 W/m-K Grade Count:8 |
Overview of materials for Polyaryletherketone (PAEK), Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyaryletherketone (PAEK), Carbon Fiber Filled". Each property range of values reported is minimum and .. |
|||
Thermal Conductivity | 0.0370 W/m-K | 0.257 BTU-in/hr-ft²-°F | ASTM E1530 |
Solvay Specialty Polymers AvaSpire® AV-848 CF30 Polyaryletherketone (PAEK)
(Unverified Data**) AvaSpire AV-848 CF30 is a 30% carbon fiber-reinforced, high-temperature, polyaryletherketone (PAEK) that has been specifically formulated to provide several performance advantages over comparable gr.. |
|||
Thermal Conductivity | 0.0370 W/m-K | 0.257 BTU-in/hr-ft²-°F | ASTM C518 |
SABIC Innovative Plastics ULTEM Foam XP080 PEI ULTEM foam is a polyetherimide based thermoplastic foam with excellent flame, smoke and toxicity performance. The material combines a high strength to weight ratio with low moisture absorption. The .. |
|||
Thermal Conductivity | 0.0370 W/m-K | 0.257 BTU-in/hr-ft²-°F | mean temp of 50°C; ISO 8301 |
Zotefoams ZOTEK® F 40 HT LS PVDF Foam Zotek® F 40 is a closed cell foam made from Arkema Kynar® PVDF manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and o.. |
|||
Thermal Conductivity | 0.0370 W/m-K | 0.257 BTU-in/hr-ft²-°F | mean temp of 10°C; ISO 8302 1991 |
Zotefoams Supazote® EM26 Lightweight Supersoft Ethylene Copolymer Foam Supazote® is a closed cell, cross-linked copolymer foam manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and outstandi.. |
|||
Thermal Conductivity | 0.0370 W/m-K | 0.257 BTU-in/hr-ft²-°F | DIN 52612 |
BASF Neopolen® P 8220 K 0.03 g/cc Core density; Expanded Polypropylene (Europe) Description: Neopolen® P 8220 K is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 8220 K.Note: In order to.. |
|||
Thermal Conductivity | 0.0370 W/m-K | 0.257 BTU-in/hr-ft²-°F | DIN 52612 |
BASF Neopolen® P 8225 K 0.03 g/cc Core density; Expanded Polypropylene (Europe) Description: Neopolen® P 8225 K is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 8225 K.Note: In order to.. |
|||
Thermal Conductivity | 0.0370 W/m-K | 0.257 BTU-in/hr-ft²-°F | DIN 52612 |
BASF Neopolen® P 9230 D 0.05 g/cc Core density; Expanded Polypropylene (Europe) Description: Neopolen® P 9230 D is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 9230 D.Note: In order to.. |
|||
Thermal Conductivity | 0.0370 W/m-K | 0.257 BTU-in/hr-ft²-°F | DIN 52612 |
BASF Neopolen® P 9335 MG 0.05 g/cc Core density; Expanded Polypropylene (Europe) Description: Neopolen® P 9333 MG is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 9333 MG.Note: In order .. |
|||
Thermal Conductivity | 0.0370 W/m-K | 0.257 BTU-in/hr-ft²-°F | DIN 52612 |
BASF Neopolen® P 9435 0.05 g/cc Core density; Expanded Polypropylene (Europe) Description: Neopolen® P 9435 is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 9435.Note: In order to mea.. |
|||
Thermal Conductivity | 0.0370 W/m-K @Temperature 50.0 °C |
0.257 BTU-in/hr-ft²-°F @Temperature 122 °F |
|
BASF Styrodur® 3035 CS Extruded Rigid Polystyrene Foam (Europe) Description: Styrodur C is the green extruded rigid polystyrene foam (XPS) from BASF. As a thermal insulation, it makes a significant contribution to climate protection by reducing CO2 emissions. Th.. |
|||
Thermal Conductivity | 0.0370 W/m-K @Thickness 100 mm |
0.257 BTU-in/hr-ft²-°F @Thickness 3.94 in |
DIN EN 13164 |
BASF Styrodur® 3035 CS Extruded Rigid Polystyrene Foam (Europe) Description: Styrodur C is the green extruded rigid polystyrene foam (XPS) from BASF. As a thermal insulation, it makes a significant contribution to climate protection by reducing CO2 emissions. Th.. |
|||
Thermal Conductivity | 0.0370 W/m-K | 0.257 BTU-in/hr-ft²-°F | ISO 8301 |
3A Composites Core Materials AIREX® R63.80 Damage Tolerant Foam AIREX® R63 is a closed-cell, linear, thermoplastic polymer foam with extremely high damage tolerance. This formula combines high elongation and excellent bond strength. AIREX® R63 is cold formable.. |
|||
Thermal Conductivity | 0.0370 W/m-K | 0.257 BTU-in/hr-ft²-°F | DIN 52612 |
BASF Neopolen® P 9225 K 0.03 g/cc Core density; Expanded Polypropylene (Europe) Description: Neopolen® P 9225 K is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 9225 K.Note: In order to.. |
|||
Thermal Conductivity | 0.0370 W/m-K | 0.257 BTU-in/hr-ft²-°F | Moisture Content: 6% |
BASF Styrodur® 4000 CS Extruded Rigid Polystyrene Foam (Europe) Description: Styrodur C is the green extruded rigid polystyrene foam (XPS) from BASF. As a thermal insulation, it makes a significant contribution to climate protection by reducing CO2 emissions. Th.. |
|||
Thermal Conductivity | 0.0370 W/m-K @Thickness 100 mm |
0.257 BTU-in/hr-ft²-°F @Thickness 3.94 in |
DIN EN 13164 |
BASF Styrodur® 4000 CS Extruded Rigid Polystyrene Foam (Europe) Description: Styrodur C is the green extruded rigid polystyrene foam (XPS) from BASF. As a thermal insulation, it makes a significant contribution to climate protection by reducing CO2 emissions. Th.. |
|||
Thermal Conductivity | 0.0370 W/m-K | 0.257 BTU-in/hr-ft²-°F | Moisture Content: 6% |
BASF Styrodur® 5000 CS Extruded Rigid Polystyrene Foam (Europe) Description: Styrodur C is the green extruded rigid polystyrene foam (XPS) from BASF. As a thermal insulation, it makes a significant contribution to climate protection by reducing CO2 emissions. Th.. |
|||
Thermal Conductivity | 0.0370 W/m-K @Thickness 100 mm |
0.257 BTU-in/hr-ft²-°F @Thickness 3.94 in |
DIN EN 13164 |
BASF Styrodur® 5000 CS Extruded Rigid Polystyrene Foam (Europe) Description: Styrodur C is the green extruded rigid polystyrene foam (XPS) from BASF. As a thermal insulation, it makes a significant contribution to climate protection by reducing CO2 emissions. Th.. |
|||
Thermal Conductivity | 0.0370 W/m-K @Thickness 50.0 mm, Temperature 50.0 °C |
0.257 BTU-in/hr-ft²-°F @Thickness 1.97 in, Temperature 122 °F |
|
BASF Styrodur® 5000 CS Extruded Rigid Polystyrene Foam (Europe) Description: Styrodur C is the green extruded rigid polystyrene foam (XPS) from BASF. As a thermal insulation, it makes a significant contribution to climate protection by reducing CO2 emissions. Th.. |
|||
Thermal Conductivity | 0.0370 W/m-K | 0.257 BTU-in/hr-ft²-°F | DIN 52612 |
BASF Neopolen® P 8015 0.03 g/cc Core density; Expanded Polypropylene (Europe) Description: Neopolen® P 8015 is expanded Polypropylene supplied in the form of beads. The cells are largely closed. Physical properties of moldings made from Neopolen® P 8015Note: In order to mea.. |
|||
Thermal Conductivity | 0.0370 W/m-K | 0.257 BTU-in/hr-ft²-°F | DIN 52612 |
BASF Neopolen® P 9230 A 0.05 g/cc Core density; Expanded Polypropylene (Europe) Description: Neopolen® P 9230 A is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 9230 A.Note: In order to.. |
|||
Thermal Conductivity | 0.0370 W/m-K | 0.257 BTU-in/hr-ft²-°F | DIN 52612 |
BASF Neopolen® P 9235 0.035 g/cc Core density; Expanded Polypropylene (Europe) Description: Neopolen® P 9235 is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 9235.Note: In order to mea.. |
|||
Thermal Conductivity | 0.0370 W/m-K | 0.257 BTU-in/hr-ft²-°F | Moisture Content: 6% |
BASF Styrodur® 2500 C Extruded Rigid Polystyrene Foam (Europe) Description: Styrodur C is the green extruded rigid polystyrene foam (XPS) from BASF. As a thermal insulation, it makes a significant contribution to climate protection by reducing CO2 emissions. Th.. |
|||
Thermal Conductivity | 0.0370 W/m-K @Temperature 50.0 °C |
0.257 BTU-in/hr-ft²-°F @Temperature 122 °F |
|
BASF Styrodur® 2500 C Extruded Rigid Polystyrene Foam (Europe) Description: Styrodur C is the green extruded rigid polystyrene foam (XPS) from BASF. As a thermal insulation, it makes a significant contribution to climate protection by reducing CO2 emissions. Th.. |
|||
Thermal Conductivity | 0.0370 W/m-K | 0.257 BTU-in/hr-ft²-°F | Moisture Content: 6% |
BASF Styrodur® 2800 C Extruded Rigid Polystyrene Foam (Europe) Description: Styrodur C is the green extruded rigid polystyrene foam (XPS) from BASF. As a thermal insulation, it makes a significant contribution to climate protection by reducing CO2 emissions. Th.. |
|||
Thermal Conductivity | 0.0370 W/m-K @Temperature 50.0 °C |
0.257 BTU-in/hr-ft²-°F @Temperature 122 °F |
|
BASF Styrodur® 2800 C Extruded Rigid Polystyrene Foam (Europe) Description: Styrodur C is the green extruded rigid polystyrene foam (XPS) from BASF. As a thermal insulation, it makes a significant contribution to climate protection by reducing CO2 emissions. Th.. |
|||
Thermal Conductivity | 0.0370 W/m-K | 0.257 BTU-in/hr-ft²-°F | Moisture Content: 6% |
BASF Styrodur® 3035 CN Extruded Rigid Polystyrene Foam (Europe) Description: Styrodur C is the green extruded rigid polystyrene foam (XPS) from BASF. As a thermal insulation, it makes a significant contribution to climate protection by reducing CO2 emissions. Th.. |
|||
Thermal Conductivity | 0.0370 W/m-K @Temperature 50.0 °C |
0.257 BTU-in/hr-ft²-°F @Temperature 122 °F |
|
BASF Styrodur® 3035 CN Extruded Rigid Polystyrene Foam (Europe) Description: Styrodur C is the green extruded rigid polystyrene foam (XPS) from BASF. As a thermal insulation, it makes a significant contribution to climate protection by reducing CO2 emissions. Th.. |
|||
Thermal Conductivity | 0.0370 W/m-K | 0.257 BTU-in/hr-ft²-°F | DIN 52612 |
BASF Neopolen® P 9435 0.035 g/cc Core density; Expanded Polypropylene (Europe) Description: Neopolen® P 9435 is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 9435.Note: In order to mea.. |