Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Thermal Conductivity = 0.0349 W/m-K Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Thermal Conductivity 0.0349 W/m-K
0.242 BTU-in/hr-ft²-°F
25g/L; KS M 3808
LG Chemical B120 EPS, Non-Flame Retardant
Feature: Expendable Polystyrene, Non-Flame RetardantApplication: Package, Fruit/Fish Box, Floats, Pad, Ice BoxCAS No. 9003-53-6 and 109-66-0Information provided by LG Chemical
Thermal Conductivity 0.0349 W/m-K
0.242 BTU-in/hr-ft²-°F
30g/L; KS M 3808
LG Chemical B240 EPS, Non-Flame Retardant
Feature: Expendable Polystyrene, Non-Flame RetardantApplication: Package, Fruit/Fish Box, Floats, Pad, Ice BoxCAS No. 9003-53-6 and 109-66-0Information provided by LG Chemical
Thermal Conductivity 0.0349 W/m-K
0.242 BTU-in/hr-ft²-°F
25g/L; KS M 3808
LG Chemical R120 EPS, Flame Retardant
Feature: Expendable Polystyrene, Flame RetardantApplication: Insulation Board, Sandwich Panel Civil Engineering & Construction MaterialsCAS No. 9003-53-6, 109-66-0, 3194-55-6 and 106-97-8Information..
Thermal Conductivity 0.0349 W/m-K
0.242 BTU-in/hr-ft²-°F
25g/L; KS M 3808
LG Chemical R160 EPS, Flame Retardant
Feature: Expendable Polystyrene, Flame RetardantApplication: Insulation Board, Sandwich Panel Civil Engineering & Construction MaterialsCAS No. 9003-53-6, 109-66-0, 3194-55-6 and 106-97-8Information..
Thermal Conductivity 0.0349 W/m-K
0.242 BTU-in/hr-ft²-°F
30g/L; KS M 3808
LG Chemical R320 EPS, Flame Retardant
Feature: Expendable Polystyrene, Flame RetardantApplication: Insulation Board, Sandwich Panel Civil Engineering & Construction MaterialsCAS No. 9003-53-6, 109-66-0, 3194-55-6 and 106-97-8Information..
Thermal Conductivity 0.0349 W/m-K
0.242 BTU-in/hr-ft²-°F
30g/L; KS M 3808
LG Chemical B320 EPS, Non-Flame Retardant
Feature: Expendable Polystyrene, Non-Flame RetardantApplication: Package, Fruit/Fish Box, Floats, Pad, Ice BoxCAS No. 9003-53-6 and 109-66-0Information provided by LG Chemical
Copyright © lookpolymers.com All Rights Reserved