Polymer Property : Thermal Conductivity = 0.0339 W/m-K Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Thermal Conductivity 0.0339 W/m-K
0.235 BTU-in/hr-ft²-°F
NOVA Chemicals Dylite® F271TN Expandable Polystyrene Resin
Highly consistent bead size, High gloss characteristics, Low energy consumption, Fast molding cycles, Food contact compliantApplications: Drinking cups (hot and cold), Noodle bowls, Take-out contai..
Thermal Conductivity 0.0339 W/m-K
0.235 BTU-in/hr-ft²-°F
NOVA Chemicals Dylite® F271TS Expandable Polystyrene Resin
Highly consistent bead size, High gloss characteristics, Low energy consumption, Fast molding cycles, Food contact compliantApplications: Drinking cups (hot and cold), Noodle bowls, Take-out contai..