Thermal Properties Metric English Comments
CTE, linear 89.0 µm/m-°C
49.4 µin/in-°F
ASTM D696
Total PS CPDS 815 High Flow, Non-Deca Polystyrene
Total Petrochemicals Polystyrene 815 is a high heat resistant, high impact Polystyrene for injection molding. It is recommended for the manufacturing of articles which require good dimensional stab..
CTE, linear 89.0 µm/m-°C
49.4 µin/in-°F
ASTM D696
Total PS CPDS 818 Easy Flow, Non-Deca Polystyrene
Total Petrochemicals Polystyrene 818 is a high heat resistant, high impact Polystyrene for injection molding and extrusion/thermoforming. It is recommended for the manufacturing of articles which r..
CTE, linear 89.0 µm/m-°C
49.4 µin/in-°F
ASTM D696
Total PS CPDS 863 High Flow Flame Retardant Deca Polystyrene
Total Petrochemicals Polystyrene 863 is a high flow, heat resistant, high impact polystyrene for injection molding. It is recommended for the manufacturing of articles which require good dimensiona..
CTE, linear 89.0 µm/m-°C
49.4 µin/in-°F
ASTM D696
Total PSC 1441 Easy Flow, High Heat Resistance Polystyrene
Total Petrochemicals Polystyrene 1441 is an easy flowing crystal polystyrene designed for extrusion or injection applications. In extrusion, it improves extruder output and thermoforming cycle time..
CTE, linear 89.0 µm/m-°C
49.4 µin/in-°F
ASTM D696
Total PS CPDS 814 UV Stabilized, Flame Retardant Polystyrene
Total Petrochemicals Polystyrene 814 is a heat resistant, UV stabilized V0 Non Deca Polystyrene for injection molding. It is recommended for the manufacturing of articles which require good dimensi..
CTE, linear 89.0 µm/m-°C
49.4 µin/in-°F
ASTM D696
Total PSC 1050 High Heat Resistance, High Molecular Weight Crystal Polystyrene
Total Petrochemicals Polystyrene 1050 is a high heat resistance, high molecular weight crystal polystyrene mainly for the extrusion industry. It is particularly useful in the production of thick sh..
CTE, linear 89.0 µm/m-°C
49.4 µin/in-°F
ASTM D696
Total PSI 2451 High Heat Resistance Impact Polystyrene
Total Petrochemicals Polystyrene 2451 is a high heat resistance, impact polystyrene for injection blow molding, thermoforming. It is recommended for the manufacturing of articles which require good..
CTE, linear 89.0 µm/m-°C
49.4 µin/in-°F
Above Tg
Epoxy Technology EPO-TEK® EJ2189-LV Electrically Conductive Epoxy
Low Viscosity, two component room temp curing conductive epoxyInformation Provided by Epoxy Technology
CTE, linear 89.0 µm/m-°C
49.4 µin/in-°F
Above Tg
Epoxy Technology EPO-TEK® N20E Electrically Conductive Paste
Product Description: EPO-TEK® N20E is a two component, electrically and thermally conductive, epoxy adhesive designed for semiconductor and electronics assembly. Its applications and field conditi..
Copyright © lookpolymers.com All Rights Reserved