Polymer Property : CTE, linear = 88.7 µm/m-°C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear 88.7 - 175 µm/m-°C
49.3 - 97.2 µin/in-°F
Average value: 153 µm/m-°C Grade Count:22
Overview of materials for Thermoplastic Polyurethane, Elastomer, Ether Grade
This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Polyurethane, Elastomer, Ether Grade". Each property range of values reported is minimum a..
CTE, linear 88.7 - 170 µm/m-°C

@Temperature -80.0 - -30.0 °C
49.3 - 94.4 µin/in-°F

@Temperature -112 - -22.0 °F
Average value: 137 µm/m-°C Grade Count:6
Overview of materials for Thermoplastic Polyurethane, Elastomer, Ether Grade
This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Polyurethane, Elastomer, Ether Grade". Each property range of values reported is minimum a..
CTE, linear 88.7 µm/m-°C

@Temperature -80.0 - -30.0 °C
49.3 µin/in-°F

@Temperature -112 - -22.0 °F
ASTM D696
Lubrizol Pellethane® 2363-75D Thermoplastic Polyurethane Elastomer
Feature: USP Class VIAvailable in Americas, Europe, Middle East, Africa, India and AsiaData provided by LubrizolLubrizol acquired the Pellethane product line from Dow in 2009.
CTE, linear 88.7 µm/m-°C

@Temperature 20.0 °C
49.3 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Dow PELLETHANE® 2103-75D Film Grade Thermoplastic Polyurethane Elastomer  (discontinued **)
Description: PELLETHANE® 2103-75D UV stabilized, polyether based thermoplastic polyurethane elastomer has excellent hydrolytic stability and excellent resistance to micro-organisms. Applications in..