Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 157 µm/m-°C @Temperature -80.0 - -30.0 °C |
87.2 µin/in-°F @Temperature -112 - -22.0 °F |
ASTM D696 |
Lubrizol Pellethane® 2363-90A Thermoplastic Polyurethane Elastomer Feature: USP Class VIAvailable in Americas, Europe, Middle East, Africa, India and AsiaData provided by LubrizolLubrizol acquired the Pellethane product line from Dow in 2009. |
|||
CTE, linear | 157 µm/m-°C | 87.2 µin/in-°F | 90 Minute UV Cure + Thermal; T>Tg; ASTM E831-93 |
3D Systems Accura® SI 40 Plastic for the SLA® 500 System Accura 40 "Ar" or "Hc" type materials - for the SLA 500 system. Mimics Nylon 6:6ApplicationsHigh temperature testing:Under hood bolt-on testingWind tunnel testingHVAC testingPrototyping and testing .. |